User contributions
Jump to navigation
Jump to search
- 21:08, 13 September 2020 diff hist -35 m E-Beam Lithography System (JEOL JBX-6300FS) deleted erroneous fiels in {tool} template
- 21:06, 13 September 2020 diff hist +49 Tool List →Other Patterning Systems: Added Raith Velion link Tag: Visual edit
- 21:05, 13 September 2020 diff hist +81 Tool List →Lithography: added FEI Sirion Nabity Tag: Visual edit
- 15:39, 13 September 2020 diff hist +1,147 COVID-19 User Policies Initial links for files - files not uploaded yet Tag: Visual edit
- 14:43, 13 September 2020 diff hist +192 N COVID-19 User Policies Initial page Tag: Visual edit
- 10:42, 8 September 2020 diff hist +1 m PECVD 1 (PlasmaTherm 790) →Recipes & Process Data Tag: Visual edit
- 10:41, 8 September 2020 diff hist -7 m PECVD 1 (PlasmaTherm 790) →Recipes & Process Information: change to Process Data Tag: Visual edit
- 10:41, 8 September 2020 diff hist +206 PECVD 1 (PlasmaTherm 790) link to recipes and data Tag: Visual edit
- 10:34, 8 September 2020 diff hist -129 m Template:Announcements removed labor day
- 14:27, 1 September 2020 diff hist 0 File:UCSB Service Agreement.pdf John d uploaded a new version of File:UCSB Service Agreement.pdf
- 14:21, 1 September 2020 diff hist 0 File:Facility-Use-MOU---Intercampus-UC-User.pdf John d uploaded a new version of File:Facility-Use-MOU---Intercampus-UC-User.pdf
- 21:30, 31 August 2020 diff hist +129 Template:Announcements labor day closure
- 11:47, 26 August 2020 diff hist +453 N S-Cubed Flexi - Operating Procedure initial secitons, draft only Tag: Visual edit
- 11:42, 26 August 2020 diff hist +238 Automated Coat/Develop System (S-Cubed Flexi) added link to SOP Tag: Visual edit
- 13:33, 24 August 2020 diff hist -551 m Template:Announcements deleted lab shutdown
- 12:17, 20 August 2020 diff hist +325 ICP Etch 1 (Panasonic E646V) link to recipes page Tag: Visual edit
- 14:23, 19 August 2020 diff hist +348 Services added Agreement "Attachment A" Tag: Visual edit
- 14:22, 19 August 2020 diff hist +87 N File:Attachment A - UCSB Master Facilities Use Agreement Labs.pdf Facilities/Service Agreement - attachment listing UCSB facilities covered
- 06:51, 19 August 2020 diff hist +386 Template:Announcements addd lab shutdown, remove ASML
- 15:06, 18 August 2020 diff hist +6 m CAIBE (Oxford Ion Mill) →Recipes: bolded recipe page li nk Tag: Visual edit
- 12:27, 18 August 2020 diff hist +45 Contact Alignment Recipes →Negative Resist (MA-6): update MA-6 NegPR flood expose Tag: Visual edit
- 12:24, 18 August 2020 diff hist +303 Contact Alignment Recipes updated powers again Tag: Visual edit
- 07:42, 18 August 2020 diff hist +224 Contact Alignment Recipes →Suss Aligners (SUSS MJB-3): updated Channel powers according ot LeeS Tag: Visual edit
- 21:29, 12 August 2020 diff hist -32 m Unaxis wafer coating procedure typos in units (nm/µm/mm), minor formatting current Tag: Visual edit
- 11:23, 11 August 2020 diff hist +86 Logitech WBS7 - Procedure for Wax Mounting with bulk Crystalbond Stick clean glass plate if wax present Tag: Visual edit
- 11:21, 11 August 2020 diff hist +421 Logitech WBS7 - Procedure for Wax Mounting with bulk Crystalbond Stick updated open/close procedure Tag: Visual edit
- 10:09, 11 August 2020 diff hist +45 m Logitech WBS7 - Procedure for Wax Mounting with bulk Crystalbond Stick unload step Tag: Visual edit
- 09:24, 11 August 2020 diff hist -14 Logitech WBS7 - Procedure for Wax Mounting with bulk Crystalbond Stick formatting to match tool menus Tag: Visual edit
- 08:12, 11 August 2020 diff hist +108 m Logitech WBS7 - Procedure for Wax Mounting with Spin-On Crystalbond attributed to Don Freeborn current Tag: Visual edit
- 07:26, 9 August 2020 diff hist +3 m Probe Station: I-V Curves with Keithley 2400 and Python Script image adjust
- 07:23, 9 August 2020 diff hist -30 m Probe Station: I-V Curves with Keithley 2400 and Python Script image adjustments Tag: Visual edit
- 07:22, 9 August 2020 diff hist +492 Probe Station: I-V Curves with Keithley 2400 and Python Script added screenshots Tag: Visual edit
- 07:21, 9 August 2020 diff hist +45 N File:Python Keithley I-V Sweep v3 icon.png current
- 07:19, 9 August 2020 diff hist +26 N File:Python Spyder - Run Button.png current
- 07:18, 9 August 2020 diff hist +44 N File:Python Keithely I-V - user settings lines.png current
- 07:16, 9 August 2020 diff hist +30 N File:Python Spyder 3.7 (anacoda) icon.png current
- 07:14, 9 August 2020 diff hist +1 m Probe Station: I-V Curves with Keithley 2400 and Python Script
- 07:14, 9 August 2020 diff hist -1 Probe Station: I-V Curves with Keithley 2400 and Python Script
- 07:14, 9 August 2020 diff hist +2,079 N Probe Station: I-V Curves with Keithley 2400 and Python Script initial procedure for Python I-V curves Tag: Visual edit
- 06:37, 9 August 2020 diff hist +143 Probe Station & Curve Tracer →Operation Procedures & Manuals: link to Python I-V Curves Tag: Visual edit
- 17:10, 29 July 2020 diff hist -16 m Fluorine ICP Etcher (PlasmaTherm/SLR Fluorine ICP) →Detailed Specifications: update LEP description Tag: Visual edit
- 17:09, 29 July 2020 diff hist 0 m Fluorine ICP Etcher (PlasmaTherm/SLR Fluorine ICP) →Recipes: spelling Tag: Visual edit
- 17:08, 29 July 2020 diff hist +6 m Fluorine ICP Etcher (PlasmaTherm/SLR Fluorine ICP) →Recipes: bolded Tag: Visual edit
- 16:00, 27 July 2020 diff hist +6 m Staff List highlight director, like other groups Tag: Visual edit
- 09:23, 27 July 2020 diff hist +30 m Goniometer (Rame-Hart A-100) - Operating Procedure →Measurement Procedure: image caption Tag: Visual edit
- 09:23, 27 July 2020 diff hist +2 m Goniometer (Rame-Hart A-100) - Operating Procedure →Measurement Procedure: indent, spacing
- 09:21, 27 July 2020 diff hist -28 Goniometer (Rame-Hart A-100) - Operating Procedure image sizing Tag: Visual edit
- 09:20, 27 July 2020 diff hist +821 N Goniometer (Rame-Hart A-100) - Operating Procedure initial page, mostly copied from "NRL Contact Angle Goniometer - Owners Manual.pdf" Tag: Visual edit
- 09:18, 27 July 2020 diff hist +33 N File:Goniometer - Reflective Sample Illustration.png current
- 09:08, 27 July 2020 diff hist +101 N File:Goniometer (Rame-Hart A-100) - Steps for Measuring v1.png current