- 17:17, 10 May 2022 diff hist +3,304 N Process Group - Process Control Data Links to all PECVD and IBD data pages Tag: Visual edit
- 17:16, 10 May 2022 diff hist +71 m Sputtering Recipes minor updates Tag: Visual edit
- 17:15, 10 May 2022 diff hist +12 Ion Beam Deposition (Veeco NEXUS) →Detailed Specifications: mentioned ITO not installed, minor formatting Tag: Visual edit
- 17:06, 10 May 2022 diff hist +30 Sputtering Recipes →Ion Beam Deposition (Veeco NEXUS): rename process control plots for clarity Tag: Visual edit
- 17:01, 10 May 2022 diff hist -23 PECVD Recipes renamed Process Control plots for clarity Tag: Visual edit
- 16:35, 10 May 2022 diff hist +135 Nanofab Staff Internal Pages →Process Group: link to Process Control Data Tag: Visual edit
- 07:24, 10 May 2022 diff hist -108 Template:Announcements F50 up
- 12:17, 5 May 2022 diff hist +24 Test Data of etching SiO2 with CHF3/CF4 updated temperature reduction comment Tag: Visual edit
- 14:32, 4 May 2022 diff hist +3 PECVD Recipes →Si3N4 [ICP-PECVD]: corrected "current process data" links, previously pointed to "HDSiO" tab Tag: Visual edit
- 08:44, 4 May 2022 diff hist +354 Template:Announcements F50 down
- 08:41, 4 May 2022 diff hist -96 Template:Announcements →F10-RT Down: fixed links
- 08:40, 4 May 2022 diff hist +724 Template:Announcements F10-RT down
- 08:17, 4 May 2022 diff hist +2 Oxford ICP Etcher - Process Control Data modified comment on "brown gunk" observation. Tag: Visual edit
- 08:16, 4 May 2022 diff hist 0 m Oxford ICP Etcher - Process Control Data →Dependence on Sample Size: set table row to header style Tag: Visual edit
- 08:13, 4 May 2022 diff hist -113 Oxford ICP Etcher - Process Control Data Add row explaining change in mask pattern Tag: Visual edit
- 16:21, 3 May 2022 diff hist -419 Template:Announcements deleted lasb closure
- 16:13, 2 May 2022 diff hist +291 S-Cubed Flexi - Operating Procedure link to DSK bake vs dev rate, recipe minor updates Tag: Visual edit
- 16:05, 2 May 2022 diff hist +2,188 S-Cubed Flexi - Operating Procedure inital procedure, and initial recipes Tag: Visual edit
- 11:14, 29 April 2022 diff hist +161 Oxford ICP Etcher - Process Control Data bolded the title row Tag: Visual edit
- 14:27, 28 April 2022 diff hist +45 Unaxis VLR Etch - Process Control Data comments on undercut profile from 3/29/22 Tag: Visual edit
- 17:48, 27 April 2022 diff hist +355 Lift-Off with I-Line Imaging Resist + LOL2000 Underlayer mentioned switching Imaging PR Tag: Visual edit
- 17:45, 27 April 2022 diff hist +23 m Lithography Recipes →Lift-Off Recipes Tag: Visual edit
- 17:39, 27 April 2022 diff hist +10 m Lithography Recipes →Lift-Off Recipes Tag: Visual edit
- 17:35, 27 April 2022 diff hist +4,054 Lift-Off with I-Line Imaging Resist + LOL2000 Underlayer wrote initial process Tag: Visual edit
- 16:34, 27 April 2022 diff hist +891 N Lift-Off with I-Line Imaging Resist + LOL2000 Underlayer added Tips, copied from DUV Liftoff page Tag: Visual edit
- 16:32, 27 April 2022 diff hist +142 Lift-Off with DUV Imaging + PMGI Underlayer corrected typo current Tag: Visual edit
- 16:29, 27 April 2022 diff hist -23 Lift-Off with DUV Imaging + PMGI Underlayer →Tips: fixed link to liftoff tutorial Tag: Visual edit
- 16:25, 27 April 2022 diff hist +633 Lithography Recipes →Lift-Off Recipes: link to I-Line Liftoff w/ LOL underlayer Tag: Visual edit
- 18:49, 26 April 2022 diff hist +72 Template:Announcements updated lab closure msg
- 15:51, 26 April 2022 diff hist +200 Unaxis VLR Etch - Process Control Data →Data - InP Ridge Etch (Unaxis VLR): updated chamber conditioning Tag: Visual edit
- 12:03, 25 April 2022 diff hist +339 Microscopes added AmScope camera model #, minor changes to liknj to Amscope section Tag: Visual edit
- 19:02, 20 April 2022 diff hist +49 Tool List →Dry Etch: added Raith Velion to Dry Etch > Ion Milling section Tag: Visual edit
- 23:31, 19 April 2022 diff hist +200 Dry Etching Recipes added Nb, Os rows, "A" for Pan1/2 Tag: Visual edit
- 23:14, 19 April 2022 diff hist +174 Thermal Processing Recipes →Bonding with Intermediate layer: link to Logitech recipes page Tag: Visual edit
- 11:54, 19 April 2022 diff hist -36 m Template:Announcements →LEXT Confocal: DOWN: fix link
- 11:53, 19 April 2022 diff hist +154 Template:Announcements →LEXT Confocal: DOWN: linked to DX-1000
- 11:51, 19 April 2022 diff hist +117 Template:Announcements updated floor cleaning closure
- 13:09, 15 April 2022 diff hist -799 Unaxis VLR Etch - Process Control Data added WorkInProgress, example table rows Tag: Visual edit
- 13:08, 15 April 2022 diff hist +1,403 N Unaxis VLR Etch - Process Control Data pasted table from Oxford ICP Tag: Visual edit: Switched
- 13:06, 15 April 2022 diff hist +9 ICP Etching Recipes →ICP-Etch (Unaxis VLR): link to Process Control Data Tag: Visual edit
- 13:02, 15 April 2022 diff hist +233 ICP Etching Recipes added Process Control Data sections for each tool Tag: Visual edit
- 11:56, 15 April 2022 diff hist +72 Process Group - Remote Fabrication Jobs fixed links to Equipment work Tag: Visual edit
- 20:51, 13 April 2022 diff hist -228 Template:Announcements Deleted DUVscope
- 20:49, 13 April 2022 diff hist +229 Template:Announcements Friday lab closure
- 17:45, 12 April 2022 diff hist +225 Dry Etching Recipes Oxford links to GaN+GaAs recipes Tag: Visual edit
- 17:43, 12 April 2022 diff hist +5 Dry Etching Recipes Oxford GaN link Tag: Visual edit
- 17:43, 12 April 2022 diff hist +1 m ICP Etching Recipes →Oxford ICP Etcher (PlasmaPro 100 Cobra) Tag: Visual edit
- 17:40, 12 April 2022 diff hist +275 ICP Etching Recipes →Oxford ICP Etcher (PlasmaPro 100 Cobra): link to GaN etch recipes Tag: Visual edit
- 13:12, 12 April 2022 diff hist -632 Template:Announcements deleted MJB, EBL service
- 12:50, 12 April 2022 diff hist +3 Test Data of Etching SiO2 with CHF3/CF4-Fluorine ICP Etcher
- 12:49, 12 April 2022 diff hist +1 Test Data of Etching SiO2 with CHF3/CF4-Fluorine ICP Etcher moved cals table to the top
- 21:08, 7 April 2022 diff hist +1,997 N ASML Stepper 3 - Job Creator initial description of usage and caveats current Tag: Visual edit
- 12:12, 7 April 2022 diff hist +105 Frequently Asked Questions →Authorship on Publications: added local technicians are put as authors Tag: Visual edit
- 10:17, 5 April 2022 diff hist +368 Template:Announcements added JEOL EBL service
- 10:48, 4 April 2022 diff hist +264 Template:Announcements added Lee's MJB service
- 12:55, 31 March 2022 diff hist +10 IBD: Calibrating Optical Thickness added approx year developed Tag: Visual edit
- 12:54, 31 March 2022 diff hist +241 IBD: Calibrating Optical Thickness minor updates Tag: Visual edit
- 12:51, 31 March 2022 diff hist 0 File:IBD SiO-FP - long 1100nm - Reflectivity Spectrum (EMpy).png John d uploaded a new version of File:IBD SiO-FP - long 1100nm - Reflectivity Spectrum (EMpy).png current
- 12:50, 31 March 2022 diff hist -42 Ion Beam Deposition (Veeco NEXUS) →Recipes: DBR Calibration-Method page created, removed the "avaialbel from process group" text Tag: Visual edit
- 12:49, 31 March 2022 diff hist +4,212 N IBD: Calibrating Optical Thickness initial version, full method described, images inserted. Tag: Visual edit
- 12:43, 31 March 2022 diff hist +97 N File:IBD 9-period DBR - Reflectivity Spectrum (EMpy).png current
- 12:36, 31 March 2022 diff hist +105 N File:IBD SiO-FP - long 1100nm - Reflectivity Spectrum (EMpy).png
- 13:30, 29 March 2022 diff hist +13 m ICP-PECVD (Unaxis VLR) →Recipes: format link to bold/underline Tag: Visual edit
- 05:20, 26 March 2022 diff hist +173 Microscopes note about turning turrets by hand Tag: Visual edit
- 05:19, 26 March 2022 diff hist +165 UCSB NanoFab Microscope Training added not about turning obj turrets by hand Tag: Visual edit
- 14:09, 23 March 2022 diff hist +341 Template:Announcements GCA service added
- 14:08, 23 March 2022 diff hist +228 Template:Announcements DUV Scope update
- 10:40, 23 March 2022 diff hist +4 m Calculators + Utilities →Example CAD File Tag: Visual edit
- 10:29, 23 March 2022 diff hist +36 Stepper 3 (ASML DUV) →Design & Fabrication Tools: Changed title to "Design Tools". JobCreator: mention remotely-uploadable, Tag: Visual edit
- 12:31, 22 March 2022 diff hist +164 m Maskless Aligner (Heidelberg MLA150) →Video Trainings: minor formatting Tag: Visual edit
- 12:29, 22 March 2022 diff hist +6 Dry Etching Recipes fixed link to FL-ICP recipes Tag: Visual edit
- 11:02, 22 March 2022 diff hist +30 m Optical Film Thickness (Nanometric) formatting "unavaialble" note Tag: Visual edit
- 10:59, 22 March 2022 diff hist +108 Optical Film Thickness (Nanometric) Note stating tool removed from lab. Tag: Visual edit
- 16:10, 21 March 2022 diff hist +66 COVID-19 User Policies masks optional, added "in progress" to full policies. Tag: Visual edit
- 16:08, 21 March 2022 diff hist -438 Template:Announcements New COVID letter from chancellor. deleted ASML maint. LEXT down.
- 17:06, 3 March 2022 diff hist +9 Chemical-Mechanical Polisher (Logitech) link to Logitech Bonder Tag: Visual edit
- 17:04, 3 March 2022 diff hist +126 Wafer Bonder (Logitech WBS7) →About: links to applicable tools Tag: Visual edit
- 12:45, 3 March 2022 diff hist 0 PECVD Recipes →Low-Stress SiN deposition (PECVD #2): bullet formatting Tag: Visual edit: Switched
- 12:31, 3 March 2022 diff hist +178 PECVD Recipes →PECVD 2 (Advanced Vacuum): link to LS-SiN plots Tag: Visual edit
- 12:28, 3 March 2022 diff hist 0 m OLD - PECVD2 Recipes John d moved page PECVD2 Recipes to OLD - PECVD2 Recipes without leaving a redirect: this page is not linked anywhere, looks like 2014 data only current
- 15:06, 1 March 2022 diff hist +2 Tool List →Packaging: fixed FLip-scribe link Tag: Visual edit
- 15:06, 1 March 2022 diff hist 0 m Wafer Cleaver (PELCO Flip-Scribe) John d moved page Wafer Cleaver (PELCO LatticeAx) to Wafer Cleaver (PELCO Flip-Scribe) without leaving a redirect: wrong name
- 14:59, 1 March 2022 diff hist +646 KLayout Design Tips Added Editing Mode Tag: Visual edit
- 09:46, 1 March 2022 diff hist +303 Wafer Cleaver (PELCO Flip-Scribe) LatticeAx --> Flip-Scribe Tag: Visual edit
- 09:43, 1 March 2022 diff hist +115 Wafer Cleaver (PELCO Flip-Scribe) links to Mfg
- 09:35, 1 March 2022 diff hist +43 N File:LatticeAx.jpg Image of PELCO LAtticeAx tool current
- 09:27, 1 March 2022 diff hist +864 N Wafer Cleaver (PELCO Flip-Scribe) new tool page
- 09:20, 1 March 2022 diff hist +243 Tool List →Packaging: added sub-categories, Linked to new LatticeAx tool Tag: Visual edit
- 08:56, 1 March 2022 diff hist +130 m Contact Aligner (SUSS MA-6) →About: minor rearrangement Tag: Visual edit
- 08:52, 1 March 2022 diff hist +62 m Contact Aligner (SUSS MA-6) linked to SB6 Bonder page Tag: Visual edit
- 16:08, 28 February 2022 diff hist +462 Step Profilometer (KLA Tencor P-7) →Detailed Specifications: added basic info Tag: Visual edit
- 08:59, 26 February 2022 diff hist +27 m ICP Etching Recipes →Old Deleted Recipes: changed "don" to "supervisor" Tag: Visual edit
- 09:44, 21 February 2022 diff hist +108 Process Group - Remote Fabrication Jobs link to takss/priority list Tag: Visual edit
- 13:44, 17 February 2022 diff hist +327 ICP-PECVD (Unaxis VLR) →About: mention SiD4 config and expense/applicaiton Tag: Visual edit
- 13:43, 17 February 2022 diff hist +116 PECVD Recipes →ICP-PECVD (Unaxis VLR): mention cost/application to optics Tag: Visual edit
- 18:03, 16 February 2022 diff hist +340 Maskless Aligner (Heidelberg MLA150) added minimum fearture size and note on DSP transparent substrates Tag: Visual edit
- 11:48, 14 February 2022 diff hist +72 N File:ASML Reticle Programming Params - MyReticleBarCode v1.xlsx John d moved page File:ASML Reticle Programming Params - MyReticleBarCode v1.xlsx to File:ASML Reticle Programming Params - MASKJAN2020 v1.xlsx: Rename to include reticle barcode in filename current Tag: New redirect
- 11:48, 14 February 2022 diff hist 0 m File:ASML Reticle Programming Params - MASKJAN2020 v1.xlsx John d moved page File:ASML Reticle Programming Params - MyReticleBarCode v1.xlsx to File:ASML Reticle Programming Params - MASKJAN2020 v1.xlsx: Rename to include reticle barcode in filename current
- 11:47, 14 February 2022 diff hist 0 File:ASML Reticle Programming Params - MASKJAN2020 v1.xlsx John d uploaded a new version of File:ASML Reticle Programming Params - MyReticleBarCode v1.xlsx
- 13:49, 11 February 2022 diff hist +53 m ICP Etch 2 (Panasonic E626I) →Recipes Tag: Visual edit