Difference between revisions of "PECVD Recipes"
Jump to navigation
Jump to search
Line 20: | Line 20: | ||
*[https://docs.google.com/spreadsheets/d/1F2pfsVnbUgaE9tsm8HZMlY6cyt-nhui0IpvGc6udhDU/edit#gid=sharing SiO<sub>2</sub> Data 2016] |
*[https://docs.google.com/spreadsheets/d/1F2pfsVnbUgaE9tsm8HZMlY6cyt-nhui0IpvGc6udhDU/edit#gid=sharing SiO<sub>2</sub> Data 2016] |
||
*[https://docs.google.com/spreadsheets/d/1MblK5Zr5Skfw0s9Hdhqr_cCwN-nCgM-ofZnsAyvVRq8/edit#gid=sharing SiO<sub>2</sub> Data 2017] |
*[https://docs.google.com/spreadsheets/d/1MblK5Zr5Skfw0s9Hdhqr_cCwN-nCgM-ofZnsAyvVRq8/edit#gid=sharing SiO<sub>2</sub> Data 2017] |
||
+ | *[https://docs.google.com/spreadsheets/d/15SocIqWQvBKSvT5oCWoZAURLaaqb9KosxCN2rueZQN8/edit#gid=sharing New Data-300nm SiO<sub>2</sub> 2017] |
||
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dDQ3VEtZQVRpdVdlbGtIZHpTNmFzNmc&usp=drive_web#gid=sharing SiO<sub>2</sub> 1000A Thickness uniformity 2014] |
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dDQ3VEtZQVRpdVdlbGtIZHpTNmFzNmc&usp=drive_web#gid=sharing SiO<sub>2</sub> 1000A Thickness uniformity 2014] |
||
*[https://docs.google.com/spreadsheets/d/1NQy-ADou6f2NBU-9jZG8KME1lOz0X5mh6HZV9_jPGes/edit#gid=sharing SiO<sub>2</sub> 1000A Thickness uniformity 2015] |
*[https://docs.google.com/spreadsheets/d/1NQy-ADou6f2NBU-9jZG8KME1lOz0X5mh6HZV9_jPGes/edit#gid=sharing SiO<sub>2</sub> 1000A Thickness uniformity 2015] |
||
*[https://docs.google.com/spreadsheets/d/1WUCm_dWpxKTjfFf1rNfLuxvwMxsyCYON_OZ3gb50L_s/edit#gid=sharing SiO<sub>2</sub> 1000A Thickness uniformity 2016] |
*[https://docs.google.com/spreadsheets/d/1WUCm_dWpxKTjfFf1rNfLuxvwMxsyCYON_OZ3gb50L_s/edit#gid=sharing SiO<sub>2</sub> 1000A Thickness uniformity 2016] |
||
*[https://docs.google.com/spreadsheets/d/1dpC_AkPD-etIH6fVuQqLfd4UMNQCEtcqhvmBpwbEncE/edit#gid=sharing SiO<sub>2</sub> 1000A Thickness uniformity 2017] |
*[https://docs.google.com/spreadsheets/d/1dpC_AkPD-etIH6fVuQqLfd4UMNQCEtcqhvmBpwbEncE/edit#gid=sharing SiO<sub>2</sub> 1000A Thickness uniformity 2017] |
||
+ | |||
== OTHER recipes: LS SiN and SiO<sub>x</sub>N<sub>y</sub> deposition (PECVD #1) == |
== OTHER recipes: LS SiN and SiO<sub>x</sub>N<sub>y</sub> deposition (PECVD #1) == |
Revision as of 10:25, 26 September 2017
Back to Vacuum Deposition Recipes.
PECVD 1 (PlasmaTherm 790)
SiN deposition (PECVD #1)
- SiN Standard Recipe
- SiN Data 2014
- SiN Data 2015
- SiN Data 2016
- SiN Data 2017
- SiN 1000A Thickness uniformity 2014
- SiN 1000A Thickness uniformity 2015
- SiN 1000A Thickness uniformity 2016
- SiN 1000A Thickness uniformity 2017
SiO2 deposition (PECVD #1)
- SiO2 Standard Recipe
- SiO2 Data 2014
- SiO2 Data 2015
- SiO2 Data 2016
- SiO2 Data 2017
- New Data-300nm SiO2 2017
- SiO2 1000A Thickness uniformity 2014
- SiO2 1000A Thickness uniformity 2015
- SiO2 1000A Thickness uniformity 2016
- SiO2 1000A Thickness uniformity 2017
OTHER recipes: LS SiN and SiOxNy deposition (PECVD #1)
- LS SiN Standard Recipe
- LS SiN Data 2014
- LS SiN 1000A Thickness uniformity 2014
- SiOxNy Standard Recipe
- SiOxNy Data 2014
- SiOxNy1000A Thickness uniformity 2014
PECVD 2 (Advanced Vacuum)
SiO2 deposition (PECVD #2)
- Oxide Standard Recipe
- Oxide Data 2014
- Oxide Data 2015
- Oxide data 2016
- Oxide Data 2017
- Oxide Thickness Uniformity 2014
- Oxide Thickness Uniformity 2015
- Oxide Thickness Uniformity 2016
- Oxide Thickness Uniformity 2017
SiN deposition (PECVD #2)
- Nitride2 Standard Recipe
- Nitride2 Data 2014
- Nitride2 Data 2015
- Nitride2 Data 2016
- Nitride2 Data 2017
- Nitride2 Thickness Uniformity 2014
- Nitride2 Thickness Uniformity 2015
- Nitride2 Thickness Uniformity 2016
- Nitride2 Thickness Uniformity 2017
- SiNx Film Stress vs LF and HF Duration Time, and Gas Flowing-rate
LS SiN deposition (PECVD #2)
- LS Nitride2 Standard Recipe
- LS Nitride2 Data 2014
- LS Nitride2 Data 2015
- LS Nitride2 Data 2016
- LS Nitride2 Data 2017
- LS Nitride2 Thickness Uniformity 2014
- LS Nitride2 Thickness Uniformity 2015
- LS Nitride2 Thickness Uniformity 2016
- LS Nitride2 Thickness Uniformity 2017
Amorphous-Si deposition (PECVD #2)
ICP-PECVD (Unaxis VLR)
SiN deposition (Unaxis VLR)
SiN (2% SiH4)
SiN (2% SiH4 - No-Ar)
SiN (2% SiH4 - No-Ar - Extra N2)
50° (pinholes) | 100° (pinholes) | 250° |
---|---|---|
SiN (100% SiH4 )
50° (pinholes) | 100° (pinholes) | 250° |
---|---|---|
SiO2 deposition (Unaxis VLR)
SiO2 (2% SiH4)
50° | 100° | 250° |
---|---|---|
SiO2 (2% SiH4 - No Ar)
50° | 100° | 250° |
---|---|---|
SiO2 (100% SiH4 HDR)
50° | 100° | 250° |
---|---|---|
SiO2 (100% SiH4 LDR)
50° | 100° | 250° |
---|---|---|
Amorphous Si (100%SiH4 Ar He)
90° | 250° |
---|---|