Difference between revisions of "Test Data of etching SiO2 with CHF3/CF4/O2 (using this recipe only for Fluorine etch of the underneath layer)"
Jump to navigation
Jump to search
(add a SEM pic) |
(Text replacement - "www.nanotech.ucsb.edu/wiki/" to "wiki.nanotech.ucsb.edu/wiki/") |
||
(4 intermediate revisions by one other user not shown) | |||
Line 15: | Line 15: | ||
|0.74 |
|0.74 |
||
|77.9 |
|77.9 |
||
− | |[https:// |
+ | |[https://wiki.nanotech.ucsb.edu/wiki/images/f/f1/SiO2_Etch_using_ICP2_with_O2.pdf] |
|- |
|- |
||
|1/28/2019 |
|1/28/2019 |
||
Line 22: | Line 22: | ||
|0.77 |
|0.77 |
||
| |
| |
||
− | |[https:// |
+ | |[https://wiki.nanotech.ucsb.edu/wiki/images/f/fa/SiO2_Etch_using_ICP2_with_O2-a.pdf] |
+ | |- |
||
+ | |3/6/2019 |
||
+ | |I21903 |
||
+ | |88.5 |
||
+ | |0.80 |
||
+ | |79.4 |
||
+ | |[https://wiki.nanotech.ucsb.edu/wiki/images/d/dc/SiO2_Etch_using_ICP2_with_O2-3-06-2019.pdf] |
||
+ | |- |
||
+ | |7/12/2019 |
||
+ | |I21906 |
||
+ | |91.9 |
||
+ | |0.69 |
||
+ | |78.1 |
||
+ | |[https://wiki.nanotech.ucsb.edu/wiki/images/0/04/I2190605.pdf] |
||
|} |
|} |