− | This system uses a laser-based scattering method to count size and distribution of particles (or other scattering defects) on a flat wafer surface. It can scan wafers in size from 4 to |
+ | This system uses a laser-based scattering method to count size and distribution of particles (or other scattering defects) on a flat wafer surface. It can scan wafers in size from 4 to 8 inches. |
+ | |||
⚫ | |||
⚫ | |||
*[[KLA-Tencor Surfscan - Standard Operating Procedure|Standard Operating Procedure]] |
*[[KLA-Tencor Surfscan - Standard Operating Procedure|Standard Operating Procedure]] |
||
− | *[ |
+ | *[https://wiki.nanotech.ucsb.edu/w/images/9/96/Surfscan-Operation-Manual.pdf Operations Manual] |
**''For detailed measurement info, it is highly recommended that you read the manual.'' |
**''For detailed measurement info, it is highly recommended that you read the manual.'' |
||
+ | *[[Wafer scanning process traveler]] |
||
− | *[[media:Surfscan-Surfscan 6200 info.pdf|Surfscan Info]] |
||
+ | *[[Glossary]] |
||
− | *[https://drive.google.com/drive/u/1/folders/1NzZgUnXo_v2WmsHIfcrsPku9o7lUICxz Standard recipes][[File:UCSBTEST.png|left|thumb|'''UCSBTEST2''' for big size particles '''(1.6-28.0)um''']][[File:UCSBTEST2 for small particles.png|left|thumb|'''UCSBTEST2''' for small size particles '''(0.16-1.6)um''']] |
||
+ | *[[Errors]] |
||
+ | |||
+ | <br /> |
||
+ | |||
+ | == Examples == |
||
+ | <br /> |
||
+ | {| class="wikitable" |
||
+ | |+A low-particle 4-inch wafer example: |
||
+ | !Gain 4: Small Particles |
||
+ | (0.160µm – 1.60µm) |
||
+ | !Gain 2: Large Particles |
||
+ | (1.60µm – 28.0µm) |
||
+ | |- |
||
+ | |[[File:Surfscan Low-Particle Example - G4.png|frameless|200x200px]] |
||
+ | |[[File:Surfscan Low-Particle Example - G2.png|frameless|200x200px]] |
||
+ | |} |
||
+ | {| class="wikitable" |
||
+ | |+A high-particle 4-inch wafer example: |
||
+ | !Gain 4: Small Particles |
||
+ | (0.160µm – 1.60µm) |
||
+ | !Gain 2: Large Particles |
||
+ | (1.60µm – 28.0µm) |
||
+ | |- |
||
+ | |''To Be Added'' |
||
+ | |''To Be Added'' |
||
+ | |} |
Revision as of 15:09, 18 November 2021
|
About
This system uses a laser-based scattering method to count size and distribution of particles (or other scattering defects) on a flat wafer surface. It can scan wafers in size from 4 to 8 inches.
Documentation
- Standard Operating Procedure
- Operations Manual
- For detailed measurement info, it is highly recommended that you read the manual.
- Wafer scanning process traveler
- Glossary
- Errors
Examples
Gain 4: Small Particles
(0.160µm – 1.60µm) |
Gain 2: Large Particles
(1.60µm – 28.0µm) |
---|---|
Gain 4: Small Particles
(0.160µm – 1.60µm) |
Gain 2: Large Particles
(1.60µm – 28.0µm) |
---|---|
To Be Added | To Be Added |