User contributions
Jump to navigation
Jump to search
- 13:52, 24 March 2020 diff hist +120 Autostep 200 Troubleshooting and Recovery →Restarting procedure Tag: Visual edit
- 13:50, 24 March 2020 diff hist +3 Autostep 200 Troubleshooting and Recovery
- 13:48, 24 March 2020 diff hist +46 Autostep 200 Troubleshooting and Recovery
- 13:46, 24 March 2020 diff hist 0 Autostep 200 Troubleshooting and Recovery Tag: Visual edit
- 13:45, 24 March 2020 diff hist +34 Autostep 200 Troubleshooting and Recovery Tag: Visual edit
- 13:30, 24 March 2020 diff hist +161 Autostep 200 Troubleshooting and Recovery RESTART POWER DOWN Tag: Visual edit
- 13:20, 24 March 2020 diff hist +3 N File:RMS control.png current
- 13:17, 24 March 2020 diff hist +13 N File:Autostep stage control.png current
- 13:15, 24 March 2020 diff hist +3 N File:Autostep DSW.png current
- 13:09, 24 March 2020 diff hist +1 Autostep 200 Troubleshooting and Recovery rest Tag: Visual edit
- 10:21, 24 March 2020 diff hist +465 Autostep 200 Troubleshooting and Recovery →Restarting procedure: add Tag: Visual edit
- 09:15, 24 March 2020 diff hist +749 Autostep 200 Troubleshooting and Recovery →Restarting procedure Tag: Visual edit
- 09:03, 24 March 2020 diff hist +20 N File:Autostep main computer switch.png current
- 09:01, 24 March 2020 diff hist +13 N File:Autostep main computer -1.png current
- 08:56, 24 March 2020 diff hist +19 N File:Autostep Cabinet .png current
- 08:48, 24 March 2020 diff hist +10 N File:Computer-2 -smart set.png current
- 08:35, 24 March 2020 diff hist +8 N File:Lower keyboard.png current
- 08:32, 24 March 2020 diff hist -2 Autostep 200 Troubleshooting and Recovery Tag: Visual edit
- 08:25, 24 March 2020 diff hist +152 Autostep 200 Troubleshooting and Recovery
- 08:22, 24 March 2020 diff hist -158 Autostep 200 Troubleshooting and Recovery →Restarting procedure Tag: Visual edit
- 08:18, 24 March 2020 diff hist +1 Autostep 200 Troubleshooting and Recovery
- 08:17, 24 March 2020 diff hist +12 Autostep 200 Troubleshooting and Recovery →Restarting procedure Tag: Visual edit
- 08:15, 24 March 2020 diff hist +163 Autostep 200 Troubleshooting and Recovery
- 08:02, 24 March 2020 diff hist +55 Autostep 200 Troubleshooting and Recovery →Restarting procedure Tag: Visual edit
- 08:00, 24 March 2020 diff hist +8 N File:Autostep 200 Upper keyboard.png current
- 07:57, 24 March 2020 diff hist +1 Autostep 200 Troubleshooting and Recovery →Restarting procedure
- 07:55, 24 March 2020 diff hist +7 Autostep 200 Troubleshooting and Recovery →Powering down Tag: Visual edit
- 22:14, 23 March 2020 diff hist +3 Autostep 200 Troubleshooting and Recovery →Powering down Tag: Visual edit
- 22:08, 23 March 2020 diff hist +237 Autostep 200 Troubleshooting and Recovery
- 21:58, 23 March 2020 diff hist -1 Autostep 200 Troubleshooting and Recovery Tag: Visual edit
- 21:56, 23 March 2020 diff hist +1,822 Autostep 200 Troubleshooting and Recovery Tag: Visual edit
- 21:41, 23 March 2020 diff hist -9 Old Training Manual current
- 14:36, 23 March 2020 diff hist +32 Autostep 200 Old training manual current
- 14:34, 23 March 2020 diff hist +88 N Autostep 200 Old training manual Created page with "[https://wiki.nanotech.ucsb.edu/w/images/5/54/Autostep200_Training_Manual_3-23-2020.pdf]" Tag: Visual edit
- 14:34, 23 March 2020 diff hist +4 Stepper 2 (AutoStep 200) →Operating Procedures Tag: Visual edit
- 14:30, 23 March 2020 diff hist 0 N File:Autostep200 Training Manual 3-23-2020.pdf current
- 14:30, 23 March 2020 diff hist +34 Stepper 2 (AutoStep 200) →Operating Procedures Tag: Visual edit
- 14:29, 23 March 2020 diff hist -145 Stepper 2 (AutoStep 200) →Operating Procedures
- 14:16, 23 March 2020 diff hist +25 Old Training Manual Tag: Visual edit
- 14:16, 23 March 2020 diff hist +17 Old Training Manual
- 14:15, 23 March 2020 diff hist +1 Old Training Manual
- 14:15, 23 March 2020 diff hist -103 Stepper 1 (GCA 6300) →Operating Procedures
- 14:14, 23 March 2020 diff hist +86 N Old Training Manual Created page with "[https://wiki.nanotech.ucsb.edu/w/images/5/5a/GCA_6300_Training_Manual-_3-23-2020.pdf]" Tag: Visual edit
- 14:13, 23 March 2020 diff hist +2 Stepper 1 (GCA 6300) →Operating Procedures
- 14:13, 23 March 2020 diff hist +24 Stepper 1 (GCA 6300) →Operating Procedures
- 14:11, 23 March 2020 diff hist 0 N File:GCA 6300 Training Manual- 3-23-2020.pdf current
- 14:05, 23 March 2020 diff hist 0 N File:GCA 6300 Training Manual-3-23-2020.pdf current
- 14:00, 23 March 2020 diff hist -97 Stepper 1 (GCA 6300) →Operating Procedures
- 14:00, 23 March 2020 diff hist +71 Stepper 1 (GCA 6300) →Operating Procedures
- 13:58, 23 March 2020 diff hist -32 Stepper 1 (GCA 6300) →Operating Procedures
- 13:58, 23 March 2020 diff hist +36 Stepper 1 (GCA 6300) →Operating Procedures
- 13:57, 23 March 2020 diff hist +16 Stepper 1 (GCA 6300) →Operating Procedures
- 13:56, 23 March 2020 diff hist -16 Stepper 1 (GCA 6300) →Operating Procedures
- 13:52, 23 March 2020 diff hist -687 Old training manual Blanked the page current Tags: Blanking Visual edit
- 13:50, 23 March 2020 diff hist +426 Old training manual
- 12:34, 23 March 2020 diff hist +134 Old training manual
- 11:39, 23 March 2020 diff hist -3 Old training manual Tag: Visual edit
- 11:38, 23 March 2020 diff hist 0 Old training manual Tag: Visual edit: Switched
- 11:37, 23 March 2020 diff hist -244 Old training manual Tag: Visual edit
- 11:37, 23 March 2020 diff hist -67 Old training manual
- 11:36, 23 March 2020 diff hist +5 Old training manual
- 11:35, 23 March 2020 diff hist +4 Old training manual Tag: Visual edit
- 11:35, 23 March 2020 diff hist +5 Old training manual Tag: Visual edit
- 11:34, 23 March 2020 diff hist +54 Old training manual Tag: Visual edit
- 11:32, 23 March 2020 diff hist +166 Old training manual Tag: Visual edit
- 11:30, 23 March 2020 diff hist 0 Old training manual
- 11:28, 23 March 2020 diff hist +60 Old training manual Tag: Visual edit
- 11:23, 23 March 2020 diff hist -210 Old training manual
- 11:22, 23 March 2020 diff hist +1 Old training manual
- 11:21, 23 March 2020 diff hist -1 Old training manual
- 11:21, 23 March 2020 diff hist +84 Old training manual
- 11:17, 23 March 2020 diff hist +4 Old training manual
- 11:17, 23 March 2020 diff hist +58 Old training manual
- 11:16, 23 March 2020 diff hist -1 Old training manual
- 11:15, 23 March 2020 diff hist +107 Old training manual
- 11:13, 23 March 2020 diff hist +2 Old training manual
- 11:13, 23 March 2020 diff hist +28 Old training manual
- 11:12, 23 March 2020 diff hist -2 Old training manual
- 11:11, 23 March 2020 diff hist +77 Old training manual
- 11:01, 23 March 2020 diff hist -60 Old training manual Blanked the page Tag: Blanking
- 10:17, 23 March 2020 diff hist +4 Old training manual Tag: Visual edit
- 10:16, 23 March 2020 diff hist +56 Old training manual Tag: Visual edit
- 10:03, 23 March 2020 diff hist -32 Old training manual Blanked the page Tag: Blanking
- 09:58, 23 March 2020 diff hist -7 GCA Old full training manual current
- 09:57, 23 March 2020 diff hist +2 GCA Old full training manual
- 09:57, 23 March 2020 diff hist -45 GCA Old full training manual
- 09:56, 23 March 2020 diff hist +34 GCA Old full training manual
- 09:53, 23 March 2020 diff hist -21 GCA Old full training manual Tag: Visual edit
- 09:53, 23 March 2020 diff hist +48 GCA Old full training manual Tag: Visual edit
- 09:52, 23 March 2020 diff hist +87 N GCA Old full training manual Created page with "Media:Example.ogg Media: GCA 6300 Stepper Training Manual- Full version 2020.pdf"
- 09:47, 23 March 2020 diff hist +32 Old training manual old stepper training Tag: Visual edit
- 09:40, 23 March 2020 diff hist +11 N File:GCA 6300 Stepper Training Manual- Full version 2020.pdf current
- 09:24, 23 March 2020 diff hist -50 Old training manual Blanked the page Tag: Blanking
- 09:00, 23 March 2020 diff hist +6 N File:GCA 6300 Stepper Training Manual- Full version 2019.pdf current
- 08:58, 23 March 2020 diff hist +1 Old training manual
- 08:57, 23 March 2020 diff hist +49 N Old training manual Created page with "GCA 6300 Stepper Training MAnual-Full version" Tag: Visual edit
- 08:53, 23 March 2020 diff hist +26 Stepper 1 (GCA 6300) →Operating Procedures
- 08:53, 23 March 2020 diff hist -90 Stepper 1 (GCA 6300) →Operating Procedures
- 08:49, 23 March 2020 diff hist -9 GCA 6300 training manual -old instructions current Tag: Visual edit
- 08:48, 23 March 2020 diff hist +35,779 N GCA 6300 training manual -old instructions Created page with "Updated 4-24-2019 GCA Stepper Training Guide & References General Information about system 1 Aligning reticle (mask) to system 2 Logging into computer/checking the system 3..."