Difference between revisions of "PECVD Recipes"
Jump to navigation
Jump to search
Line 13: | Line 13: | ||
== SiO<sub>2</sub> deposition (PECVD #1) == |
== SiO<sub>2</sub> deposition (PECVD #1) == |
||
*[[media:|SiO<sub>2</sub> Deposition Recipe]] |
*[[media:|SiO<sub>2</sub> Deposition Recipe]] |
||
− | *[[media:PECVD1 SiO2 Data-March 2014 SiO2 Data.pdf|SiO<sub>2</sub> |
+ | *[[media:PECVD1 SiO2 Data-March 2014 SiO2 Data.pdf|SiO<sub>2</sub> Data( Deposition rate, Refractive Index, Stress, HF etch rate)]] |
Revision as of 12:08, 21 March 2014
Back to Vacuum Deposition Recipes.
PECVD 1 (PlasmaTherm 790)
SiN deposition (PECVD #1)
- SiN Standard Recipe
- SiN Data (Deposition rate, Refractive index, Stress, HF etch rate)
- SiN 1000A Thickness uniformity 2014
- SiN Data March 2014
SiO2 deposition (PECVD #1)
- [[media:|SiO2 Deposition Recipe]]
- SiO2 Data( Deposition rate, Refractive Index, Stress, HF etch rate)
SiOxNy deposition (PECVD #1)
PECVD 2 (Advanced Vacuum)
SiN deposition (PECVD #2)
SiO2 deposition (PECVD #2)
Amorphous-Si deposition (PECVD #2)
ICP-PECVD (Unaxis VLR)
SiN deposition (Unaxis VLR)
SiN (2% SiH4)
SiN (2% SiH4 - No-Ar)
50° | 100° | 250° |
---|---|---|
SiN (2% SiH4 - No-Ar - Extra N2)
50° | 100° | 250° |
---|---|---|
SiN (100% SiH4 )
50° | 100° | 250° |
---|---|---|
SiO2 deposition (Unaxis VLR)
SiO2 (2% SiH4)
50° | 100° | 250° |
---|---|---|
SiO2 (2% SiH4 - No Ar)
50° | 100° | 250° |
---|---|---|
SiO2 (100% SiH4 HDR)
50° | 100° | 250° |
---|---|---|
SiO2 (100% SiH4 LDR)
50° | 100° | 250° |
---|---|---|
Amorphous Si (100%SiH4 Ar He)
90° | 250° |
---|---|