== SiN deposition (PECVD #2) ==
 
*[[media:New Advanced PECVD-Nitride2 300C standard recipe.pdf|Nitride2 Standard Recipe]]
 
*[[media:ADV PECVD NITRIDE2-Data April 2014.pdf|Nitride2 Data (Deposition Rate, Refractive Index, Stress, HF etch rate)]]
 
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dDE0R3FlenNPa2txNmRldTczMXZNNnc#gid=sharing Nitride2 Data 2014]
 
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dERkYm85bGtYQVpjVk5GTGJuMkg2anc&usp=drive_web#gid=sharing Nitride2 Thickness uniformity 2014]
 
 
*Deposition Rate: ≈ 9.0 nm/min
 
*Refractive Index: ≈ 1.952
 
*Stress ≈ 484MPa
 
 
 
== SiO<sub>2</sub> deposition (PECVD #2) ==
 
== SiO<sub>2</sub> deposition (PECVD #2) ==
 
*[[media:Advanced PECVD OXIDE 300C standard recipe OXIDE Standard Recipe.pdf|Oxide Standard Recipe]]
 
*[[media:Advanced PECVD OXIDE 300C standard recipe OXIDE Standard Recipe.pdf|Oxide Standard Recipe]]
Line 40: Line 30:
 
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dDRjSHEtYUZRUTg4azE2U0JGUTg2M1E#gid=sharing Oxide Thickness uniformity 2014]
 
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dDRjSHEtYUZRUTg4azE2U0JGUTg2M1E#gid=sharing Oxide Thickness uniformity 2014]
   
 
== SiN deposition (PECVD #2) ==
*Deposition Rate: ≈ 28.0 nm/min
 
 
*[[media:New Advanced PECVD-Nitride2 300C standard recipe.pdf|Nitride2 Standard Recipe]]
*Refractive Index: ≈ 1.472
 
 
*[[media:ADV PECVD NITRIDE2-Data April 2014.pdf|Nitride2 Data (Deposition Rate, Refractive Index, Stress, HF etch rate)]]
*Stress ≈ -270MPa
 
 
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dDE0R3FlenNPa2txNmRldTczMXZNNnc#gid=sharing Nitride2 Data 2014]
 
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dERkYm85bGtYQVpjVk5GTGJuMkg2anc&usp=drive_web#gid=sharing Nitride2 Thickness uniformity 2014]
   
 
==LS SiN deposition (PECVD #2) ==
 
==LS SiN deposition (PECVD #2) ==
Line 51: Line 43:
 
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dENSak1ZNnVaVTFEQTBzdDJMSDlDTFE&usp=drive_web#gid=1=sharing LS Nitride2 Thickness uniformity 2014]
 
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dENSak1ZNnVaVTFEQTBzdDJMSDlDTFE&usp=drive_web#gid=1=sharing LS Nitride2 Thickness uniformity 2014]
   
*Deposition Rate: ≈ 8.34 nm/min
 
*Refractive Index: ≈ 1.932
 
*Stress ≈ -45MPa
 
   
 
== Amorphous-Si deposition (PECVD #2) ==
 
== Amorphous-Si deposition (PECVD #2) ==

Revision as of 11:47, 9 January 2015

Back to Vacuum Deposition Recipes.

PECVD 1 (PlasmaTherm 790)

SiN deposition (PECVD #1)

SiO2 deposition (PECVD #1)

SiOxNy deposition (PECVD #1)

PECVD 2 (Advanced Vacuum)

SiO2 deposition (PECVD #2)

SiN deposition (PECVD #2)

LS SiN deposition (PECVD #2)


Amorphous-Si deposition (PECVD #2)

ICP-PECVD (Unaxis VLR)

SiN deposition (Unaxis VLR)

SiN (2% SiH4)

50° 100° 250°

SiN (2% SiH4 - No-Ar)

50° 100° 250°

SiN (2% SiH4 - No-Ar - Extra N2)

50° 100° 250°

SiN (100% SiH4 )

50° 100° 250°

SiO2 deposition (Unaxis VLR)

SiO2 (2% SiH4)

50° 100° 250°

SiO2 (2% SiH4 - No Ar)

50° 100° 250°

SiO2 (100% SiH4 HDR)

50° 100° 250°

SiO2 (100% SiH4 LDR)

50° 100° 250°

Amorphous Si (100%SiH4 Ar He)

90° 250°