Thermal Evap 2 (Solder)
|
About
Materials Table
Materials Table
| ||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|
Material | Symbol | Density, g/cm3 | Z Ratio | Tooling, % | Comments | |||||||
Aluminum | Al | 2.70 | 1.08 | Antimony | Sb | 2.70 | 0.768 | |||||
Arsenic | As | 5.73 | 0.996 | |||||||||
Beryllium | Be | 1.85 | 0.543 | |||||||||
Boron | B | 2.54 | 0.389 | |||||||||
Cadmium | Cd | 8.64 | 0.682 | |||||||||
Cadmium sulfide | CdS | 4.83 | 1.02 | |||||||||
Cadmium telluride | CdTe | 5.85 | 0.980 | |||||||||
Calcium fluoride | CaF2 | 3.18 | 0.775 | |||||||||
Carbon (graphite) | C | 2.25 | 3.26 | |||||||||
Chromium | Cr | 7.20 | 0.305 | 155 | ||||||||
Cobalt | Co | 8.71 | 0.343 | |||||||||
Copper | Cu | 8.93 | 0.437 | |||||||||
Gallium | Ga | 5.93 | 0.593 | |||||||||
Gallium Arsenide | GaAs | 5.31 | 1.59 | |||||||||
Germanium | Ge | 5.35 | 0.516 | |||||||||
Gold | Au | 19.30 | 0.381 | |||||||||
Indium | In | 7.30 | 0.841 | 120 | ||||||||
Indium antimonide | InSb | 5.76 | 0.769 | |||||||||
Iridium | Ir | 22.4 | 0.129 | |||||||||
Iron | Fe | 7.86 | 0.349 | |||||||||
Lead | Pb | 11.3 | 1.13 | |||||||||
Lead sulfide | PbS | 7.50 | 0.566 | |||||||||
Lithium fluoride | LiF | 2.64 | 0.774 | |||||||||
Magnesium | Mg | 1.74 | 1.61 | |||||||||
Magnesium oxide | MgO | 3.58 | 0.411 | |||||||||
Magnesium Fluoride | MgF2 | 3.00 | 0.427 | |||||||||
Manganese | Mn | 7.20 | 0.377 | |||||||||
Manganese(II) Sulfide | MnS | 3.99 | 0.94 | |||||||||
Mercury | Hg | 13.46 | 0.74 | |||||||||
Molybdenum | Mo | 10.2 | 0.257 | |||||||||
Nickel | Ni | 8.91 | 0.331 | |||||||||
Niobium | Nb | 8.57 | 0.493 | |||||||||
Niobium(V) Oxide | Nb2O5 | 4.47 | ||||||||||
Palladium | Pd | 12.0 | 0.357 | |||||||||
Platinum | Pt | 21.4 | 0.245 | |||||||||
Potasium Cloride | KCl | 1.98 | 2.05 | |||||||||
Selenium | Se | 4.82 | 0.864 | |||||||||
Silicon | Si | 2.32 | 0.712 | |||||||||
Silicon(II) Oxide | SiO | 2.13 | 0.87 | |||||||||
Silicon dioxide (fused quarz) | SiO2 | 2.20 | 1.07 | |||||||||
Silver | Ag | 10.5 | 0.529 | |||||||||
Silver bromide | AgBr | 6.47 | 1.18 | |||||||||
Silver chloride | AgCl | 5.56 | 1.32 | |||||||||
Sodium | Na | 0.97 | 4.8 | |||||||||
Sodium chloride | NaCl | 2.17 | 1.57 | |||||||||
Tantalum | Ta | 16.6 | 0.262 | |||||||||
Tantalum(IV) oxide | Ta2O5 | 8.2 | 0.30 | |||||||||
Tin | Sn | 7.30 | 0.724 | |||||||||
Titanium | Ti | 4.50 | 0.628 | |||||||||
Titanium (IV) Oxide | TiO2 | 4.26 | 0.40 | |||||||||
Titanium Oxide | TiO | 4.90 | N/A | |||||||||
Tangsten | W | 19.3 | 0.163 | |||||||||
Tangsten carbide | WC | 15.6 | 0.151 | |||||||||
Zinc | Zn | 7.04 | 0.514 | |||||||||
Zinc Oxide | Zn | 5.61 | 0.556 | |||||||||
Zinc Sulfide | ZnS | 4.09 | 0.775 | |||||||||
Zirconium | Zr | 6.51 | 0.60 | |||||||||
Zirconium Oxide | ZrO2 | 5.6 |