+ | Thermal evaporator #2 is the designated "Solder" evaporator. The tool is used primarily for solder materials including Gold, Indium and Tin. Use this tool for materials with low melting temperatures, or for materials that have a high risk of contamination in the e-beam evaporators. |
||
− | write something... |
||
− | |||
− | = Materials Table = |
||
− | Work on this page... For the materials tables, please visit the [[E-Beam_Evaporation_Recipes#Materials_Table_(E-Beam #1)|E-Beam Recipe Page]]. |
||
= Detailed Specifications = |
= Detailed Specifications = |
||
+ | Wafers up to 12" can be mounted. |
||
− | work on this page... |
||
=Documentation= |
=Documentation= |
||
− | *[[ |
+ | *[[ media: Thermal Evaporator2.pdf|Operating Instructions]] |
− | |||
− | |||
− | |||
= Materials Table = |
= Materials Table = |
||
+ | For the materials tables, please visit the [[Thermal_Evaporation_Recipes#Materials_Table_(Thermal Evaporator #1)|Thermal Evaporation Recipe Page]]. |
||
− | |||
+ | ==Data== |
||
− | {| border="1" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" class="collapsible collapsed wikitable" |
||
+ | [[Thermal Evaporation Recipes]] |
||
− | |- |
||
− | ! colspan=6 width=1300 height=35 bgcolor="#D0E7FF" align="center"|<div style="font-size: 150%;">Materials Table</div> |
||
− | |- bgcolor="#D0E7FF" |
||
− | ! width="45" bgcolor="#D0E7FF" align="center" | '''Material''' |
||
− | ! width="45" bgcolor="#D0E7FF" align="center" | '''Symbol''' |
||
− | ! width="45" bgcolor="#D0E7FF" align="center" | '''Density, g/cm3''' |
||
− | ! width="45" bgcolor="#D0E7FF" align="center" | '''Z Ratio''' |
||
− | ! width="45" bgcolor="#D0E7FF" align="center" | '''Tooling, %''' |
||
− | ! width="100" bgcolor="#D0E7FF" align="center" | '''Comments''' |
||
− | |- |
||
− | |Aluminum |
||
− | |Al |
||
− | |2.70 |
||
− | |1.08 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Antimony |
||
− | |Sb |
||
− | |6.620 |
||
− | |0.768 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Arsenic |
||
− | |As |
||
− | |5.73 |
||
− | |0.996 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Beryllium |
||
− | |Be |
||
− | |1.85 |
||
− | |0.543 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Boron |
||
− | |B |
||
− | |2.54 |
||
− | |0.389 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Cadmium |
||
− | |Cd |
||
− | |8.64 |
||
− | |0.682 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Cadmium sulfide |
||
− | |CdS |
||
− | |4.83 |
||
− | |1.02 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Cadmium telluride |
||
− | |CdTe |
||
− | |5.85 |
||
− | |0.980 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Calcium fluoride |
||
− | |CaF<sub>2</sub> |
||
− | |3.18 |
||
− | |0.775 |
||
− | | |
||
− | |Used often |
||
− | |- |
||
− | |Carbon (graphite) |
||
− | |C |
||
− | |2.25 |
||
− | |3.26 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Chromium |
||
− | |Cr |
||
− | |7.20 |
||
− | |0.305 |
||
− | |155 |
||
− | |Used often |
||
− | |- |
||
− | |Cobalt |
||
− | |Co |
||
− | |8.71 |
||
− | |0.343 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Copper |
||
− | |Cu |
||
− | |8.93 |
||
− | |0.437 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Gallium |
||
− | |Ga |
||
− | |5.93 |
||
− | |0.593 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Gallium Arsenide |
||
− | |GaAs |
||
− | |5.31 |
||
− | |1.59 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Germanium |
||
− | |Ge |
||
− | |5.35 |
||
− | |0.516 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Gold |
||
− | |Au |
||
− | |19.30 |
||
− | |0.381 |
||
− | | |
||
− | |Used often |
||
− | |- |
||
− | |Indium |
||
− | |In |
||
− | |7.30 |
||
− | |0.841 |
||
− | |120 |
||
− | |Used often |
||
− | |- |
||
− | |Indium antimonide |
||
− | |InSb |
||
− | |5.76 |
||
− | |0.769 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Iridium |
||
− | |Ir |
||
− | |22.4 |
||
− | |0.129 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Iron |
||
− | |Fe |
||
− | |7.86 |
||
− | |0.349 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Lead |
||
− | |Pb |
||
− | |11.3 |
||
− | |1.13 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Lead sulfide |
||
− | |PbS |
||
− | |7.50 |
||
− | |0.566 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Lithium fluoride |
||
− | |LiF |
||
− | |2.638 |
||
− | |0.778 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Magnesium |
||
− | |Mg |
||
− | |1.74 |
||
− | |1.61 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Magnesium oxide |
||
− | |MgO |
||
− | |3.58 |
||
− | |0.411 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Magnesium Fluoride |
||
− | |MgF<sub>2</sub> |
||
− | |3.00 ( should be 3.18) |
||
− | |0.427( should be 0.637) |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Manganese |
||
− | |Mn |
||
− | |7.20 |
||
− | |0.377 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Manganese(II) Sulfide |
||
− | |MnS |
||
− | |3.99 |
||
− | |0.94 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Mercury |
||
− | |Hg |
||
− | |13.46 |
||
− | |0.74 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Molybdenum |
||
− | |Mo |
||
− | |10.2 |
||
− | |0.257 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Nickel |
||
− | |Ni |
||
− | |8.91 |
||
− | |0.331 |
||
− | | |
||
− | |Used often |
||
− | |- |
||
− | |Niobium |
||
− | |Nb |
||
− | |8.578 |
||
− | |0.492 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Niobium(V) Oxide |
||
− | |Nb<sub>2</sub>O<sub>5</sub> |
||
− | |4.47 |
||
− | |*1.00 |
||
− | | |
||
− | |*z ratio has not been established |
||
− | |- |
||
− | |Palladium |
||
− | |Pd |
||
− | |12.0 |
||
− | |0.357 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Platinum |
||
− | |Pt |
||
− | |21.4 |
||
− | |0.245 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Potasium Cloride |
||
− | |KCl |
||
− | |1.98 |
||
− | |2.05 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Selenium |
||
− | |Se |
||
− | |4.82 |
||
− | |0.864 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Silicon |
||
− | |Si |
||
− | |2.32 |
||
− | |0.712 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Silicon(II) Oxide |
||
− | |SiO |
||
− | |2.13 |
||
− | |0.87 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Silicon dioxide (fused quarz) |
||
− | |SiO<sub>2</sub> |
||
− | |2.20 |
||
− | |1.07 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Silver |
||
− | |Ag |
||
− | |10.5 |
||
− | |0.529 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Silver bromide |
||
− | |AgBr |
||
− | |6.47 |
||
− | |1.18 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Silver chloride |
||
− | |AgCl |
||
− | |5.56 |
||
− | |1.32 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Sodium |
||
− | |Na |
||
− | |0.97 |
||
− | |4.8 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Sodium chloride |
||
− | |NaCl |
||
− | |2.17 |
||
− | |1.57 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Tantalum |
||
− | |Ta |
||
− | |16.6 |
||
− | |0.262 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Tantalum(IV) oxide |
||
− | |Ta<sub>2</sub>O<sub>5</sub> |
||
− | |8.2 |
||
− | |0.30 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Tin |
||
− | |Sn |
||
− | |7.30 |
||
− | |0.724 |
||
− | | |
||
− | |Used often |
||
− | |- |
||
− | |Titanium |
||
− | |Ti |
||
− | |4.50 |
||
− | |0.628 |
||
− | | |
||
− | |Used often |
||
− | |- |
||
− | |Titanium (IV) Oxide |
||
− | |TiO<sub>2</sub> |
||
− | |4.26 |
||
− | |0.40 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Titanium Oxide |
||
− | |TiO |
||
− | |4.90 |
||
− | |*1.00 |
||
− | | |
||
− | |* z ratio not established |
||
− | |- |
||
− | |Tungsten |
||
− | |W |
||
− | |19.3 |
||
− | |0.163 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Tungsten carbide |
||
− | |WC |
||
− | |15.6 |
||
− | |0.151 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Zinc |
||
− | |Zn |
||
− | |7.04 |
||
− | |0.514 |
||
− | | |
||
− | |Used often |
||
− | |- |
||
− | |Zinc Oxide |
||
− | |ZnO |
||
− | |5.61 |
||
− | |0.556 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Zinc Sulfide |
||
− | |ZnS |
||
− | |4.09 |
||
− | |0.775 |
||
− | | |
||
− | | |
||
− | |- |
||
− | |Zirconium |
||
− | |Zr |
||
− | |6.51 |
||
− | |0.60 |
||
− | | |
||
− | |Should be 6.49 |
||
− | |- |
||
− | |Zirconium Oxide |
||
− | |ZrO<sub>2</sub> |
||
− | |5.6 |
||
− | |1.001 |
||
− | | |
||
− | | |
||
− | |- |
Revision as of 10:47, 24 May 2017
|
About
Thermal evaporator #2 is the designated "Solder" evaporator. The tool is used primarily for solder materials including Gold, Indium and Tin. Use this tool for materials with low melting temperatures, or for materials that have a high risk of contamination in the e-beam evaporators.
Detailed Specifications
Wafers up to 12" can be mounted.
Documentation
Materials Table
For the materials tables, please visit the Thermal Evaporation Recipe Page.