YES Recipe Screenshots: STD-O2

From UCSB Nanofab Wiki
Jump to navigation Jump to search
STD-O2-100C-3KW-15min
Header Steps
screenshot of STD-O2-100C-3KW-15min - header
STD-O2-100C-3KW-15min - header
screenshot of STD-O2-100C-3KW-15min - steps
STD-O2-100C-3KW-15min - steps
STD-O2-180C-3KW-30sec
Header Steps
screenshot of STD-O2-180C-3KW-30sec - header
STD-O2-180C-3KW-30sec - header
screenshot of STD-O2-180C-3KW-30sec - steps
STD-O2-180C-3KW-30sec - steps