(Created page with " XeF2 Etch (Xetch) Jump to: navigation, search XeF2 Etch (Xetch) XeF2.jpg Tool Type Dry Etch Location Bay 2 Supervisor Don Freeborn Supervisor Phone (805) 893-3918x216 Sup...")
 
 
(One intermediate revision by one other user not shown)
Line 1: Line 1:
  +
{{tool|{{PAGENAME}}
XeF2 Etch (Xetch)
 
 
|picture=XeF2.jpg
Jump to: navigation, search
 
 
|type = Dry Etch
XeF2 Etch (Xetch)
 
 
|super= Don Freeborn
XeF2.jpg
 
  +
|phone=(805)839-3918x216
Tool Type Dry Etch
 
Location Bay 2
+
|location=Bay 2
  +
|email=freeborn@ece.ucsb.edu
Supervisor Don Freeborn
 
  +
|description = XeF<sub>2</sub> Gas Etcher
Supervisor Phone (805) 893-3918x216
 
  +
|manufacturer = [http://www.xactix.com/ Xactix Inc]
Supervisor Cell
 
  +
|materials =
Supervisor E-Mail dfreeborn@ece.ucsb.edu
 
  +
|toolid=31
Description XeF2 Gas Etcher
 
  +
}}
Manufacturer Xactix Inc
 
  +
= About =
XeF2 Etch (Xetch) Recipes
 
 
The applications of this tool are mainly in MEMS-device fabrication areas (releasing a MEMS structure by etching a sacrificial layer below), in which Si or Ge or even some metals, such as Mo, can be isotropically dry etched using gaseous XeF<sub>2</sub> (no plasma enhancement or heating is needed) with the use of photoresist or SiO<sub>2</sub> or Al as an etch mask at room temperature. For users who want to etch through or very deep into a Si wafer, they should use the Si Deep RIE tool in the lab. The XeF<sub>2</sub> etch process is a purely chemical one and usually results in a rough etched surface. The tool is operated in a pulsed mode in which the etch chamber is repeatedly filled with XeF<sub>2</sub> gas and, then, pumped out (to 0.3 Torr). You can also add N<sub>2</sub> gas, together with XeF<sub>2</sub> gas, into the etch chamber for some applications. There is a microscope attached to this tool, with which you can monitor the etch process of your sample. You can change the number of etch cycles during a run, which will be effective in that run. Also, you can manually stop a run based on microscope observations.
Sign up for this tool
 
[edit] About
 
   
 
=Documentation=
The applications of this tool are mainly in MEMS-device fabrication areas (releasing a MEMS structure by etching a sacrificial layer below), in which Si or Ge or even some metals, such as Mo, can be isotropically dry etched using gaseous XeF2 (no plasma enhancement or heating is needed) with the use of photoresist or SiO2 or Al as an etch mask at room temperature. For users who want to etch through or very deep into a Si wafer, they should use the Si Deep RIE tool in the lab. The XeF2 etch process is a purely chemical one and usually results in a rough etched surface. The tool is operated in a pulsed mode in which the etch chamber is repeatedly filled with XeF2 gas and, then, pumped out (to 0.3 Torr). You can also add N2 gas, together with XeF2 gas, into the etch chamber for some applications. There is a microscope attached to this tool, with which you can monitor the etch process of your sample. You can change the number of etch cycles during a run, which will be effective in that run. Also, you can manually stop a run based on microscope observations.
 
 
*[[media:|System Manual]]
[edit] Documentation
 
  +
*[[media:|System Manual]]
 
 
*[[media:|Si Etching Profile & Results]]
System Manual
 
Si Etching Profile & Results
 

Latest revision as of 16:41, 30 January 2014

Vapor HF Etch (uETCH)
XeF2.jpg
Tool Type Dry Etch
Location Bay 2
Supervisor Don Freeborn
Supervisor Phone (805) 893-7975
Supervisor E-Mail dfreeborn@ece.ucsb.edu
Description XeF2 Gas Etcher
Manufacturer Xactix Inc
Dry Etch Recipes
Sign up for this tool


About

The applications of this tool are mainly in MEMS-device fabrication areas (releasing a MEMS structure by etching a sacrificial layer below), in which Si or Ge or even some metals, such as Mo, can be isotropically dry etched using gaseous XeF2 (no plasma enhancement or heating is needed) with the use of photoresist or SiO2 or Al as an etch mask at room temperature. For users who want to etch through or very deep into a Si wafer, they should use the Si Deep RIE tool in the lab. The XeF2 etch process is a purely chemical one and usually results in a rough etched surface. The tool is operated in a pulsed mode in which the etch chamber is repeatedly filled with XeF2 gas and, then, pumped out (to 0.3 Torr). You can also add N2 gas, together with XeF2 gas, into the etch chamber for some applications. There is a microscope attached to this tool, with which you can monitor the etch process of your sample. You can change the number of etch cycles during a run, which will be effective in that run. Also, you can manually stop a run based on microscope observations.

Documentation

  • [[media:|System Manual]]
  • [[media:|System Manual]]