=Materials Table=
+
==Materials Table==
   
 
{| border="1" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" class="collapsible collapsed wikitable"
 
{| border="1" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" class="collapsible collapsed wikitable"
 
|-
 
|-
! colspan=8 width=1300 height=35 bgcolor="#D0E7FF" align="center"|<div style="font-size: 150%;">Materials Table</div>
+
! colspan=8 width=1300 height=35 bgcolor="#D0E7FF" align="center"|<div style="font-size: 150%;">Materials Table for Thermal Evaporator #1</div>
 
|- bgcolor="#D0E7FF"
 
|- bgcolor="#D0E7FF"
 
! width="45" bgcolor="#D0E7FF" align="center" | '''Material'''
 
! width="45" bgcolor="#D0E7FF" align="center" | '''Material'''
Line 67: Line 67:
 
|15.86
 
|15.86
 
|23.96
 
|23.96
||
 
 
|
 
|
 
|
 
|
 
|
|Used often
 
 
|
 
|-
 
|-
 
|Gold/Palladium
 
|Gold/Palladium
Line 76: Line 76:
 
|16.40
 
|16.40
 
|23.80
 
|23.80
||
 
 
|
 
|
 
|
 
|
  +
|
|Used often
 
  +
|
 
|-
 
|-
Gold/Zinc
+
|Gold/Zinc
 
|Au.95/Zn.05
 
|Au.95/Zn.05
 
|18.72
 
|18.72
Line 89: Line 89:
 
|
 
|
 
|
 
|
|Used often
 
 
|-
 
|-
Gold/Zinc
+
|Gold/Zinc
 
|Au.90/Zn.10
 
|Au.90/Zn.10
 
|18.07
 
|18.07
Line 99: Line 98:
 
|
 
|
 
|
 
|
|Used often
 
 
|-
 
|-
  +
|Magnezium
|Magnesium
 
 
|Mg
 
|Mg
 
|1.74
 
|1.74
Line 182: Line 180:
 
|
 
|
 
|-
 
|-
  +
|Strontium Fluoride
|StrontiumFluoride
 
 
|SrF<sub>2
 
|SrF<sub>2
 
|4.28
 
|4.28
Line 201: Line 199:
 
|-
 
|-
 
|ITO(IndiumTinOxide)
 
|ITO(IndiumTinOxide)
|In<sub>2O<sub>3-SnO<sub>2
+
|In<sub>2</sub>O<sub>3</sub> - SnO<sub>2
|5.43-7.14
+
|6.43-7.14
 
|0.841
 
|0.841
 
|
 
|
Line 210: Line 208:
 
|-
 
|-
 
|Permalloy
 
|Permalloy
|Ni<sub>0.1Fe<sub>0.2
+
|Ni<sub>0.1</sub>Fe<sub>0.2</sub>
 
|8.7
 
|8.7
 
|26.40
 
|26.40
Line 217: Line 215:
 
|0.1
 
|0.1
 
|
 
|
|-
+
|}
   
 
=[[Thermal Evaporator 2]]=
 
=[[Thermal Evaporator 2]]=
   
= Materials Table =
+
== Materials Table ==
   
 
{| border="1" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" class="collapsible collapsed wikitable"
 
{| border="1" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" class="collapsible collapsed wikitable"
 
|-
 
|-
! colspan=6 width=1300 height=35 bgcolor="#D0E7FF" align="center"|<div style="font-size: 150%;">Materials Table</div>
+
! colspan=6 width=1300 height=35 bgcolor="#D0E7FF" align="center"|<div style="font-size: 150%;">Materials Table for Thermal Evaporator #2</div>
 
|- bgcolor="#D0E7FF"
 
|- bgcolor="#D0E7FF"
 
! width="45" bgcolor="#D0E7FF" align="center" | '''Material'''
 
! width="45" bgcolor="#D0E7FF" align="center" | '''Material'''
Line 646: Line 644:
 
|
 
|
 
|
 
|
|-
+
|}
  +
  +
== In Deposition (Thermal Evaporator 2) ==
  +
*[[media:Thermal evaporator 2-new Sheet1.pdf|Indium evaporation Data]]