Line 149: Line 149:
 
|0.841
 
|0.841
 
|120
 
|120
 +
|
 +
|-
 +
|Indium antimonide
 +
|InSb
 +
|5.76
 +
|0.769
 +
|
 +
|
 +
|-
 +
|Iridium
 +
|Ir
 +
|22.4
 +
|0.129
 +
|
 +
|
 +
|-
 +
|Iron
 +
|Fe
 +
|7.86
 +
|0.349
 +
|
 
|
 
|
 
|-
 
|-