Difference between revisions of "Template:Recipe"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
(comment help)
(format noinclide text)
Line 2: Line 2:
 
Use the Definition List syntax, where ; denotes a title and : denotes a new line for the list under that item.
 
Use the Definition List syntax, where ; denotes a title and : denotes a new line for the list under that item.
 
-->
 
-->
<noinclude>The recipe shown here is just a placeholder - please replace this info with your own. This text won't show up in the final page.</noinclude>
+
<noinclude>===The recipe shown here is just a placeholder - please replace this info with your own. This text won't show up in the final page.===</noinclude>
 
==Recipe==
 
==Recipe==
   

Revision as of 14:54, 3 August 2017

The recipe shown here is just a placeholder - please replace this info with your own. This text won't show up in the final page.

Recipe

Recipe Name
SiOVert_MadeUp
Tool
Panasonic ICP #2
Description
This recipe is made up, and deposits glass with lots of holes in it.
Recipe Parameters
Ar = 20 sccm
O2 = 10 sccm
Pressure = 50 mT
RF = 200 W
Temperature = 200°C
Dep Rate
200 nm/min or 12,000 nm/sec
Notes
Make sure sample is inside out before loading into tool.
This recipe usually doesn't work.
Film will etch in HF

Characterization

Al-thickness-variation-with-rate.jpg