LAB CLOSED
Due to the fire in the hills above Goleta and brownouts from it, we are closing the nanofab for the night. We will be in tomorrow morning to evaluate the safety of restarting all the tools. Please check email for updates. // John d 22:26, 6 July 2018 (PDT)
PlasmaTherm SLR: Down
The SLR fluorine etcher is down, the turbo has failed. Will work on it on Monday. // John d 22:04, 6 July 2018 (PDT)
PECVD#1: Software Upgrade
We are going to upgrade the computer and software on PECVD#1 in 2–3 weeks. The tool will be down for three to five days. Once the upgrade is complete, everyone will need to be retrained on the new software. You should start planning accordingly, if you use this tool. We will send out an email when we know the exact dates. // John d 15:05, 20 June 2018 (PDT)
RIE#5: SiCl4 Issue
We have a flow rate problem on the SiCl4 gas line. You can only flow the SiCl4 for 5 minutes and then you have to wait 5 minutes before you flow it again. So in order to to do a 10 minute Etch you will have to do it in three steps flow 5 mi, wait 5mi, then flow 5min. // John d 17:22, 15 June 2018 (PDT)