+ | =====Stepper #3 (ASML DUV) - PM Moved to 5/6 – 5/10===== |
+ | We are postponing the Maintenance date to May 6th – 10th. |
||
− | We are continuing to work our way through the issue plaguing this system. Unfortunately running at lower power did not work. We will send updates more regularly to keep you all informed. |
||
+ | On the week of May 6th, ASML Engineers will be performing preventative maintenance, please plan your work around the tool being down at that time. |
||
⚫ | |||
− | Tony |
||
⚫ | |||
⚫ | |||
+ | The tool is working properly at this time and is now available for use. Thank you for your patience in regard to this matter. |
||
− | =====MLA 150 Service Next Week - REMINDER===== |
||
⚫ | |||
− | The MLA 150 will be down for a service visit from Tuesday February 6th to Thursday February 8th. The tool should be available in the evenings and it's possible the work will be completed by the end of Wednesday. |
||
+ | =====DI and Waste Water systems===== |
||
− | Here's the schedule for when the tool will be unavailable: |
||
+ | DI and Waste Water systems will be down for upgrade April 5th and 6th. |
||
− | |||
⚫ | |||
− | Tues (2/6): 11:30 am - 5 pm |
||
⚫ | |||
− | |||
+ | The board we were waiting on arrived, but it did not resolve the tool issue. We are working with Panasonic on the next steps. |
||
− | Wed (2/7): 8 am - 5 pm |
||
⚫ | |||
− | |||
− | Thurs (2/8) 8 am - 5 pm (if needed). |
||
− | |||
− | -Lee |
||
− | |||
⚫ | |||
− | |||
− | =====MJB-3 Service Next Week - REMINDER===== |
||
− | The MJB-3s will be unavailable Thursday Feb. 8th for their annual service visit. |
||
− | |||
− | //[[User:Mehalana v|Vraj Mehalana]] 10:37, 1 February 2024 (PST) |
||
− | |||
− | =====MA6 Service Next Week - REMINDER===== |
||
− | The MA-6 will be unavailable Tuesday Feb 6th from 8 am to roughly 5 pm for its annual service visit. |
||
− | |||
− | The issue with the backside camera magnification getting stuck will be addressed during the visit. |
||
− | |||
− | -Lee |
||
− | |||
− | //[[User:Mehalana v|Vraj Mehalana]] 10:37, 1 February 2024 (PST) |
||
⚫ | |||
− | RIE 5 is up except for processes that use SiCl4. |
||
− | |||
⚫ | |||
− | =====Dry Etch, Si Deep RIE (PlasmaTherm DSEIII) - DSE Update===== |
||
− | We received most of the chamber assembly replacement parts today. We are still waiting on the lamps and chamber o-rings which are scheduled to be delivered in the next couple of days. Once we have all the parts, we'll start to reassemble the chamber. |
||
− | |||
− | I'll send out an update in the next 2-3 days. |
||
− | |||
− | Thanks, |
||
− | //[[User:Mehalana v|Vraj Mehalana]] 10:58, 5 February 2024 (PST) |
||
− | |||
⚫ | |||
− | The tool remains down. We did not find any "smoking gun" with the PC but did find that the PC's power supply had a non functional fan and the power supply did not test as good (granted it would still power up the PC). We will continue troubleshooting the PC issue in the morning. |
||
− | |||
− | -Lee |
||
− | |||
⚫ | |||
− | =====EBeam3 Planned Maintenance 2/7/24 - 2/8/24===== |
||
− | EBeam3 is scheduled to be down starting at 8:00am on 2/7/24 through 4:00pm on 2/8//24 so that we can install the new transfer arm. |
||
− | |||
− | Please plan accordingly. |
||
− | |||
− | //[[User:Mehalana v|Vraj Mehalana]] 09:28, 26 January 2024 (PST) |
||
− | =====Oxford Cobra: Software bugs===== |
||
− | The latest revision of software has several bugs: see email for details. We are working with Oxford to resolve via software upgrade. |
||
− | // [[User:John_d|Demis D. John]] 10:08, 17 January 2024 (PST) |
||
=====Job Opening: Process Engineer===== |
=====Job Opening: Process Engineer===== |
||
Line 69: | Line 24: | ||
=====Lab Access Changes: Symmetry App===== |
=====Lab Access Changes: Symmetry App===== |
||
Card/Iris scanner access is still currently enabled. However we will be moving to a smartphone-based access system. '''IMPORTANT''': check your email to setup the new smartphone access system, so you will be ready when we switch to the new system. Look for an email titled '''''"Invitation to Access Symmetry App"'''''. |
Card/Iris scanner access is still currently enabled. However we will be moving to a smartphone-based access system. '''IMPORTANT''': check your email to setup the new smartphone access system, so you will be ready when we switch to the new system. Look for an email titled '''''"Invitation to Access Symmetry App"'''''. |
||
− | |||
// [[User:John d|John d]] 13:49, 7 November 2023 (PST) |
// [[User:John d|John d]] 13:49, 7 November 2023 (PST) |
||
Revision as of 20:15, 10 April 2024
Stepper #3 (ASML DUV) - PM Moved to 5/6 – 5/10
We are postponing the Maintenance date to May 6th – 10th. On the week of May 6th, ASML Engineers will be performing preventative maintenance, please plan your work around the tool being down at that time.
//Vraj Mehalana 09:42, 5 April 2024 (PDT)
ALD Oxford UP
The tool is working properly at this time and is now available for use. Thank you for your patience in regard to this matter. //Vraj Mehalana 13:48, 19 March 2024 (PDT)
DI and Waste Water systems
DI and Waste Water systems will be down for upgrade April 5th and 6th. //Vraj Mehalana 11:55, 18 March 2024 (PDT)
ICP1 Down
The board we were waiting on arrived, but it did not resolve the tool issue. We are working with Panasonic on the next steps. //Vraj Mehalana 14:17, 1 March 2024 (PST)
Job Opening: Process Engineer
The Nanofab has a current job opening for a Process/Wafer-Fab Engineer, see the NanoFab Job Openings page for details.
//Demis D. John 14:52, 30 October 2023 (PDT)
Lab Access Changes: Symmetry App
Card/Iris scanner access is still currently enabled. However we will be moving to a smartphone-based access system. IMPORTANT: check your email to setup the new smartphone access system, so you will be ready when we switch to the new system. Look for an email titled "Invitation to Access Symmetry App". // John d 13:49, 7 November 2023 (PST)
Wafer Bonder, (Suss SB6-8E)