Step Profilometer (KLA Tencor P-7)

From UCSB Nanofab Wiki
Revision as of 23:06, 4 April 2024 by John d (talk | contribs) (updated specs)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search
Step Profilometer (KLA Tencor P-7)
KLA-Tencor-P7 Photo.JPG
Location Bay 4
Tool Type Inspection, Test and Characterization
Manufacturer KLA Tencor
Description Surface Profilometer

Primary Supervisor Bill Millerski
(805) 893-2655
wmillerski@ucsb.edu

Secondary Supervisor

Aidan Hopkins


Recipes N/A


About

The KLA-Tencor P7 profilometer is a stylus profilometer that drags a stylus across the wafer surface with controlled pressure, aligned via microcope, and measures the step-heights of surface features during the measurement. The system has a motor-controlled stage for X/Y/Rotation, and is typically used to measure step heights in single areas on various sample sizes frmo small pieces to 4-inch wafers. It can be programmed to scan multiple locations on a single wafer or 3D areas topography.

Detailed Specifications

  • Probe Tip: 2um radius and 60° angle
  • Maximum wafer size: 6-inch
  • 1D Profile and 2D Raster Scanning
  • Automated Measurement Routines

Instructions