13:58, 15 April 2014 PECVD1-SiN-standard recipe 2014.pdf (file) 298 KB   1
14:29, 15 April 2014 PECVD1 SIN Data-April 2014 SIN data.pdf (file) 117 KB   1
14:42, 15 April 2014 PECVD1-SiO2-standard recipe 2014.pdf (file) 299 KB   1
14:44, 15 April 2014 PECVD1 SiO2 Data-April 2014 SiO2 Data.pdf (file) 116 KB   1
08:11, 16 April 2014 AdvPECVD-Nitride2 300C standard recipe.pdf (file) 42 KB   1
08:15, 16 April 2014 AdvPECVD OXIDE 300C standard recipe.pdf (file) 42 KB   1
08:18, 16 April 2014 AdvPECVD-LS Nitride2 300C standard recipe.pdf (file) 43 KB   1
09:53, 1 October 2014 PECVD1-SiON-recipe 2014 LS SION recipe.pdf (file) 1.24 MB   1
14:24, 10 October 2014 PECVD1-SiON-recipe 2014 LS SION recipe LS SION recipe.pdf (file) 1.24 MB   1
14:02, 17 October 2014 Dirty platen photos.pdf (file) 2.65 MB   1
10:42, 21 October 2014 PECVD1-LS SIN-Turner05recipe 2014 LS SIN recipe.pdf (file) 733 KB   1
15:23, 3 December 2014 PECVD1-LS SION recipe 2014.pdf (file) 1.24 MB   1
15:37, 5 December 2014 PECVD1-LS SIN recipe 2014.pdf (file) 1.03 MB   1
09:25, 10 December 2014 PECVD1-SiN-standard recipe 2014 SiN standard recipe.pdf (file) 298 KB   1
09:32, 10 December 2014 PECVD1-SiN standard recipe 2014.pdf (file) 299 KB   1
10:22, 10 December 2014 PECVD1-SiO2-standard recipe 2014 SiO2 standard recipe.pdf (file) 299 KB   1
11:18, 10 December 2014 PECVD1-LS SION-recipe2014 LS SION recipe.pdf (file) 1.24 MB   1
09:52, 11 December 2014 NewAdvPECVD OXIDE 300C standard recipe.pdf (file) 653 KB   1
11:01, 11 December 2014 NewAdvPECVD-Nitride2 300C standard recipe.pdf (file) 373 KB   1
11:10, 11 December 2014 Photos Sheet1.pdf (file) 4.23 MB   1
13:41, 11 December 2014 NewAdvPECVD-LS Nitride2 300C standard recipe.pdf (file) 378 KB   1
13:58, 11 December 2014 NewPECVD1-SiN-standard recipe 2014.pdf (file) 299 KB   1
13:59, 11 December 2014 NewPECVD1-SiO2-standard recipe 2014.pdf (file) 299 KB   1
14:03, 8 January 2015 New PECVD1-SiO2-standard recipe 2014 SiO2 standard recipe.pdf (file) 594 KB   1
14:04, 8 January 2015 New PECVD1-SiN-standard recipe 2014 SiN standard recipe.pdf (file) 595 KB   1
14:31, 8 January 2015 New PECVD1-LS SION-recipe 2014 LS SION recipe.pdf (file) 1.59 MB   1
15:11, 8 January 2015 New PECVD1-LS SIN-Turner05recipe 2014 LS SIN recipe.pdf (file) 1.38 MB   1
10:54, 9 January 2015 New Adv PECVD OXIDE 300C standard recipe OXIDE Standard Recipe.pdf (file) 653 KB   1
10:56, 9 January 2015 New Adv PECVD-Nitride2 300C standard recipe Nitride2 Standard Recipe.pdf (file) 373 KB   1
10:57, 9 January 2015 New Adv PECVD-LS Nitride2 300C standard recipe LS Nitride2 standard recipe.pdf (file) 378 KB   1
14:10, 8 May 2015 GCA 6300 Training Manual-4-10-2015.pdf (file) 257 KB   1
14:14, 8 May 2015 Autostep 200 Training Manual-4-10-15 .pdf (file) 252 KB   1
08:53, 12 April 2016 Surfscan-Surfscan 6200 info.pdf (file) 114 KB   1
09:07, 12 April 2016 Surfscan.jpg (file) 162 KB   1
08:52, 23 May 2017 Adv PECVD-LS Nitride2 300C standard recipe .pdf (file) 379 KB   1
13:43, 23 May 2017 Sputter5 SiO2 2017 SiO2 film.pdf (file) 86 KB   1
09:54, 24 May 2017 Thermal evaporator 2 Sheet1.pdf (file) 31 KB   1
12:17, 24 May 2017 Thermal evaporator 2.pdf (file) 20 KB   1
12:28, 24 May 2017 Thermal evaporator 2-new Sheet1.pdf (file) 20 KB   1
07:43, 20 October 2017 AdvPECVD-LS Nitride2 300C standard recipe LS Nitride2 standard recipe.pdf (file) 380 KB   2
07:52, 20 October 2017 New AdvPECVD-LS Nitride2 300C standard recipe LS Nitride2 standard recipe.pdf (file) 380 KB   1
09:32, 27 December 2018 STD LSNitride2 recipe new info.pdf (file) 37 KB   2
13:15, 2 January 2019 STD LSNitride2 recipe new info 1-2-2019 Dep.recipe.pdf (file) 349 KB   2
13:16, 2 January 2019 STD LSNitride2 12-14-18 recipe.pdf (file) 349 KB   1
13:48, 2 January 2019 18.pdf (file) 400 KB   1
14:03, 2 January 2019 STD LSNitride2 5-9-18.pdf (file) 400 KB   1
14:26, 2 January 2019 STD Nitride 5-9-18.pdf (file) 209 KB   1
14:39, 2 January 2019 STD Nitride 5-9-18 Dep.recipe.pdf (file) 209 KB   1
14:49, 2 January 2019 STD Oxide 5-9-18 Dep.recipe.pdf (file) 238 KB   1
15:03, 2 January 2019 STD SiO2 5-9-18.pdf (file) 239 KB   1