User contributions
Jump to navigation
Jump to search
- 09:35, 8 September 2018 diff hist 0 Lab Rules OLD 2018 uploading new lab policy doc
- 08:36, 6 September 2018 diff hist 0 N File:BCB-rework.pdf current
- 08:36, 6 September 2018 diff hist +52 Lithography Recipes →Chemical Datasheets: Added BCB rework doc from DOW to list
- 17:37, 4 September 2018 diff hist -99 Chemical List - OLD 2018-09-05 →UNSORTED
- 17:29, 31 August 2018 diff hist +99 Chemical List - OLD 2018-09-05 Testing link to MSDS folder Tag: Visual edit
- 17:08, 21 August 2018 diff hist -14 m Template:Announcements →Ebeam#2: heater repair scheduled
- 17:06, 21 August 2018 diff hist -8 m Template:Announcements update EB2
- 08:03, 21 August 2018 diff hist -81 Wet Benches →General Information
- 11:09, 3 August 2018 diff hist -34,565 Lab Rules OLD 2018 deleted all except pdf. Old verion on _backup Tag: Visual edit
- 11:07, 3 August 2018 diff hist +35,139 N Lab Rules backup Created page with "For a printable PDF version of the Lab Rules, please '''CLICK HERE''' While working in the Nanofab, you are surr..." current
- 15:34, 7 June 2018 diff hist +90 Template:Announcements
- 14:22, 6 June 2018 diff hist -107 Template:Announcements
- 11:06, 4 June 2018 diff hist -101 Template:Announcements
- 14:52, 26 May 2018 diff hist -20 Template:Announcements
- 11:05, 26 May 2018 diff hist +200 Template:Announcements
- 10:41, 26 May 2018 diff hist +29 Template:Announcements
- 10:41, 26 May 2018 diff hist +168 Template:Announcements
- 10:38, 26 May 2018 diff hist -28 Template:Announcements
- 09:54, 25 May 2018 diff hist -30 Vacuum Deposition Recipes minor link edit sputter5 Tag: Visual edit
- 09:52, 25 May 2018 diff hist +19 m Vacuum Deposition Recipes link to sputter5 recipes Tag: Visual edit
- 09:49, 25 May 2018 diff hist -140 Sputtering Recipes
- 17:27, 24 May 2018 diff hist -34 Template:Announcements →Stepper #2: Up
- 17:25, 24 May 2018 diff hist -248 Template:Announcements →PECVD#2: Open Soon
- 16:49, 14 May 2018 diff hist +147 Vacuum Deposition Recipes Fixed ALD Links to proper headings Tag: Visual edit
- 16:44, 14 May 2018 diff hist +10 Vacuum Deposition Recipes Pt ALD link Tag: Visual edit
- 16:37, 10 May 2018 diff hist -404 Template:Announcements deleted old messaged, updated PECVD2
- 16:34, 10 May 2018 diff hist -95 Template:Announcements →PECVD#2: Down, Retraining required
- 11:46, 20 April 2018 diff hist -178 Template:Announcements
- 17:18, 19 April 2018 diff hist -731 Template:Announcements
- 17:16, 19 April 2018 diff hist -156 Template:Announcements
- 16:50, 19 April 2018 diff hist 0 m Wet Etching Recipes →The Master Table of Wet Etching (Include All Materials) Tag: Visual edit
- 16:43, 19 April 2018 diff hist -80 ICP Etching Recipes →GaSb Etch (Unaxis VLR) Tag: Visual edit
- 14:35, 19 April 2018 diff hist 0 N File:BCB-adhesion.pdf current
- 14:34, 19 April 2018 diff hist +56 m Lithography Recipes →Chemical Datasheets Tag: Visual edit
- 13:14, 19 April 2018 diff hist -5 m RIE 5 (PlasmaTherm) →About Tag: Visual edit
- 14:18, 3 April 2018 diff hist -56 m Lithography Recipes →Chemical Datasheets Tag: Visual edit
- 14:16, 3 April 2018 diff hist +7 m Lithography Recipes →Chemical Datasheets Tag: Visual edit
- 14:14, 3 April 2018 diff hist -57 m Lithography Recipes →Chemical Datasheets Tag: Visual edit
- 14:12, 3 April 2018 diff hist +256 m E-Beam 1 (Sharon) →About Tag: Visual edit
- 14:10, 3 April 2018 diff hist +47 m E-Beam Evaporation Recipes →Materials Table (E-Beam #1) Tag: Visual edit
- 09:23, 29 March 2018 diff hist +4 Template:Announcements →ASML: Up
- 09:22, 29 March 2018 diff hist +2 Template:Announcements →ASML: Up
- 09:21, 29 March 2018 diff hist -89 Template:Announcements →ASML: Leveling Error
- 15:11, 17 January 2018 diff hist +67 Dry Etching Recipes
- 15:02, 17 January 2018 diff hist 0 N File:10-Si Etch Single Step Smooth Sidewall DSEIII.pdf current
- 15:02, 17 January 2018 diff hist 0 N File:10-Si Etch Bosch DSEIII.pdf current
- 15:01, 17 January 2018 diff hist +144 ICP Etching Recipes →DSEIII_(PlasmaTherm/Deep_Silicon_Etcher)
- 17:32, 11 December 2017 diff hist -19 Template:Announcements →GCA 6300 Stepper #1
- 17:31, 11 December 2017 diff hist -28 Template:Announcements →Announcements
- 13:07, 11 December 2017 diff hist -32 Template:Announcements →Announcements
- 15:46, 28 November 2017 diff hist 0 N Category:Pages generating RSS feeds Created blank page current
- 11:02, 28 November 2017 diff hist -30 Template:News
- 11:00, 28 November 2017 diff hist -10 Template:News
- 10:58, 28 November 2017 diff hist -29 Template:News
- 10:56, 28 November 2017 diff hist -5 Template:News
- 15:20, 6 November 2017 diff hist +116 Dry Etching Recipes
- 15:18, 6 November 2017 diff hist +10 Dry Etching Recipes
- 15:16, 6 November 2017 diff hist +98 Dry Etching Recipes
- 15:13, 6 November 2017 diff hist -5 ICP Etching Recipes →DSEIII_(PlasmaTherm/Deep_Silicon_Etcher)
- 15:12, 6 November 2017 diff hist -1 ICP Etching Recipes
- 15:10, 6 November 2017 diff hist +142 ICP Etching Recipes
- 15:03, 6 November 2017 diff hist +56 Dry Etching Recipes Tag: Visual edit: Switched
- 10:45, 6 November 2017 diff hist 0 DSEIII (PlasmaTherm/Deep Silicon Etcher)
- 10:43, 6 November 2017 diff hist +2,424 N DSEIII (PlasmaTherm/Deep Silicon Etcher) Created page with "{{tool|{{PAGENAME}} |picture=DSEIII.jpg |type = Dry Etch |super= Don Freeborn |phone= 805-893-3918x216 |location=Bay 2 |email=freeborn@ece.ucsb.edu |description = Deep Silicon..."
- 10:34, 6 November 2017 diff hist +47 Tool List →Dry Etch
- 11:18, 10 October 2017 diff hist -9 Tube Furnace (Tystar 8300) →See Also
- 17:04, 29 September 2017 diff hist +66 Template:News
- 16:52, 29 September 2017 diff hist -8 MediaWiki:Sidebar
- 16:51, 29 September 2017 diff hist +15 MediaWiki:Sidebar
- 16:49, 29 September 2017 diff hist +70 MediaWiki:Sidebar
- 16:32, 29 September 2017 diff hist +1 Stepper 3 (ASML DUV) →About
- 10:47, 22 September 2017 diff hist -26 Template:Links
- 17:01, 21 September 2017 diff hist -25 m Vacuum Deposition Recipes Tag: Visual edit
- 17:01, 21 September 2017 diff hist -50 m Vacuum Deposition Recipes Tag: Visual edit
- 11:30, 8 September 2017 diff hist +4 Lithography Recipes →Chemical Datasheets Tag: Visual edit: Switched
- 11:26, 8 September 2017 diff hist -1 Lithography Recipes Tag: Visual edit: Switched
- 11:18, 8 September 2017 diff hist -71 Lithography Recipes →Chemical Datasheets
- 11:17, 8 September 2017 diff hist 0 File:UV26-Positive-Resist-Datasheet.pdf Thibeault uploaded a new version of File:UV26-Positive-Resist-Datasheet.pdf current
- 11:16, 8 September 2017 diff hist 0 N File:UV26-Positive-Resist-Datasheet.pdf
- 11:16, 8 September 2017 diff hist +53 Lithography Recipes →Chemical Datasheets
- 11:10, 8 September 2017 diff hist 0 m Vacuum Deposition Recipes Tag: Visual edit: Switched
- 14:48, 12 June 2017 diff hist +52 Lithography Recipes →Photolithography Recipes
- 14:37, 12 June 2017 diff hist 0 N File:NR9-1000PY-AS200-stepperrecipe.pdf current
- 14:36, 12 June 2017 diff hist +319 Stepper Recipes
- 14:31, 12 July 2016 diff hist 0 N File:Survey052016.pdf current
- 14:30, 12 July 2016 diff hist +20 Template:News
- 14:28, 12 July 2016 diff hist +51 Template:News
- 16:59, 3 June 2016 diff hist +40 ICP Etch 2 (Panasonic E626I) →Detailed Specifications
- 16:58, 3 June 2016 diff hist +92 Fluorine ICP Etcher (PlasmaTherm/SLR Fluorine ICP) →Detailed Specifications
- 16:55, 3 June 2016 diff hist 0 ICP Etching Recipes
- 16:52, 3 June 2016 diff hist 0 N File:10-Si Etch Bosch Release DRIE.pdf current
- 16:51, 3 June 2016 diff hist +114 ICP Etching Recipes →Si Deep RIE (PlasmaTherm/Bosch Etch)
- 14:33, 3 June 2016 diff hist -47 Stepper 3 (ASML DUV) →About
- 14:31, 3 June 2016 diff hist +359 Stepper 3 (ASML DUV) →About
- 14:25, 3 June 2016 diff hist +318 Stepper 3 (ASML DUV) →About
- 11:51, 3 June 2016 diff hist 0 N File:ASML Job Set-Up Guide simple v1.pdf current
- 11:49, 3 June 2016 diff hist +96 Stepper 3 (ASML DUV) →Operating Procedures
- 12:01, 22 February 2016 diff hist 0 Sputtering Recipes →Sputter 4 (AJA ATC 2200-V)
- 11:36, 22 February 2016 diff hist +130 Sputtering Recipes →Sputter 3 (AJA ATC 2000-F)
- 15:37, 16 December 2015 diff hist +60 Dry Etching Recipes