- 15:59, 7 July 2022 diff hist +134 Dry Etching Recipes added LiNbO3, SU8, BCB Tag: Visual edit
- 15:50, 7 July 2022 diff hist +121 Template:Recipe Table Explanation note that this template is no longer used current
- 15:48, 7 July 2022 diff hist +159 Lithography Recipes →Photolithography Recipes: removed recipe table explanation template Tag: Visual edit
- 15:46, 7 July 2022 diff hist +158 Dry Etching Recipes smaller fonts to make table more obvious Tag: Visual edit
- 15:44, 7 July 2022 diff hist +17 m Vacuum Deposition Recipes →Process Control Data: smaller font current Tag: Visual edit
- 15:44, 7 July 2022 diff hist +157 Vacuum Deposition Recipes →Deposition Tools/Materials Table: removed tempalte for smaller table explanation Tag: Visual edit
- 10:35, 7 July 2022 diff hist -1 m Ellipsometer (Woollam)
- 10:34, 7 July 2022 diff hist -19 Ellipsometer (Woollam) updated to tool2, added Aidan + Demis as super/super2
- 16:58, 6 July 2022 diff hist +263 MLA150 - Troubleshooting →Solution for 3-4 inch wafers: added CAD reduction by ≥10mm Tag: Visual edit
- 16:05, 6 July 2022 diff hist +11 Wet Etching Recipes force TOC above link to Master Table
- 16:04, 6 July 2022 diff hist -192 Wet Etching Recipes moved and emphasized link to master table. Tag: Visual edit: Switched
- 11:52, 6 July 2022 diff hist +22 Maskless Aligner (Heidelberg MLA150) added 2nd supervisor via {{tool2}} template, Lee Sawyer
- 08:16, 6 July 2022 diff hist +2,838 UCSB NanoFab Microscope Training Added Optical Filters & DIC sections Tag: Visual edit
- 08:04, 6 July 2022 diff hist +46 N File:Microscopes - DIC filters and light path.png current
- 07:49, 6 July 2022 diff hist +52 N File:Microscopes - Filter Out position-detent.png current
- 10:18, 5 July 2022 diff hist -64 Template:Announcements updateD ASML
- 09:45, 5 July 2022 diff hist +61 DUMMY TOOL testing Tag: Visual edit
- 17:19, 4 July 2022 diff hist +49 m Packaging Recipes →Wax-Mounting to Carrier: writing creidts Tag: Visual edit
- 17:16, 4 July 2022 diff hist +2,819 Packaging Recipes →Mounting/Unmounting Samples: added “wax mounting to carrier” Tag: Visual edit
- 07:47, 1 July 2022 diff hist +69 Direct-Write Lithography Recipes →Maskless Aligner (Heidelberg MLA150): links to MJB/MA6 for Flood exp Tag: Visual edit
- 21:58, 30 June 2022 diff hist +211 Direct-Write Lithography Recipes →Positive Resist (MLA150): clarify “PEB” Tag: Visual edit
- 09:44, 28 June 2022 diff hist -179 Template:Announcements ASML update, system up, software fixed
- 18:59, 27 June 2022 diff hist +41 Template:Announcements asml UP, editing issue
- 03:09, 27 June 2022 diff hist +37 Template:Tool2 →Options
- 03:08, 27 June 2022 diff hist +148 Template:Tool2
- 03:06, 27 June 2022 diff hist +134 Template:Tool2 added example image
- 03:02, 27 June 2022 diff hist +41 N File:TOOL template - example image.png example of the tool infobox current
- 03:00, 27 June 2022 diff hist +21 Template:Tool2 added <includeonly>
- 02:56, 27 June 2022 diff hist +7 Template:StaffInfoSecondary DJ current
- 02:56, 27 June 2022 diff hist +15 Template:StaffInfo DJ current
- 02:55, 27 June 2022 diff hist +5 Template:StaffContactInfo DJ
- 02:55, 27 June 2022 diff hist 0 Template:StaffContactInfo DJ
- 02:54, 27 June 2022 diff hist +6 Template:StaffContactInfo DJ
- 02:54, 27 June 2022 diff hist -59 Template:StaffContactInfo DJ
- 02:54, 27 June 2022 diff hist +65 Template:StaffContactInfo DJ updated instructions
- 02:45, 27 June 2022 diff hist -1 DUMMY TOOL
- 02:44, 27 June 2022 diff hist +91 Template:Tool2 added classes to each table, for eventual CSS
- 02:41, 27 June 2022 diff hist 0 Template:Tool2
- 02:41, 27 June 2022 diff hist -38 Template:Tool2 Undo revision 160087 by John d (talk) Tag: Undo
- 02:40, 27 June 2022 diff hist +266 Template:Tool2 added row style="border-bottom: 1px solid grey"
- 02:38, 27 June 2022 diff hist +38 Template:Tool2 messing with tr borders
- 02:36, 27 June 2022 diff hist 0 Template:Tool2
- 02:35, 27 June 2022 diff hist +18 DUMMY TOOL
- 02:34, 27 June 2022 diff hist -18 DUMMY TOOL
- 02:34, 27 June 2022 diff hist -4 m Template:Tool2
- 02:33, 27 June 2022 diff hist +18 DUMMY TOOL added Super2=Ning Cao
- 02:32, 27 June 2022 diff hist +41 Template:Tool2 put "super2" into an {{if super2}}
- 02:31, 27 June 2022 diff hist -20 DUMMY TOOL remoed super2 to see what happens
- 02:28, 27 June 2022 diff hist -152 Template:StaffContactInfo DJ updated editing instructions
- 02:22, 27 June 2022 diff hist -183 m Template:StaffContactInfo DJ
- 02:17, 27 June 2022 diff hist 0 Template:Tool2 move table close to end
- 02:14, 27 June 2022 diff hist +10 Template:Tool2 add "SUM Link" col title
- 02:13, 27 June 2022 diff hist 0 Template:Tool2 testing: SUM width 200
- 02:11, 27 June 2022 diff hist -24 Template:Tool2 Undo revision 160071 by John d (talk) Tag: Undo
- 02:09, 27 June 2022 diff hist +3 Template:Tool2 Undo revision 160072 by John d (talk) Tag: Undo
- 02:09, 27 June 2022 diff hist -3 m Template:Tool2
- 02:06, 27 June 2022 diff hist +24 Template:Tool2 add SUM Link col title
- 02:05, 27 June 2022 diff hist -63 Template:Tool2 move SUM link out of table, use HR instead
- 02:03, 27 June 2022 diff hist +79 Template:Tool2 Undo revision 160068 by John d (talk) Tag: Undo
- 02:02, 27 June 2022 diff hist -79 Template:Tool2 SUM link in same table
- 02:01, 27 June 2022 diff hist 0 m Template:Tool2
- 02:01, 27 June 2022 diff hist -38 Template:Tool2 add col title for "recipes"
- 01:57, 27 June 2022 diff hist 0 m Template:Tool2
- 01:56, 27 June 2022 diff hist +8 m Template:Tool2
- 01:55, 27 June 2022 diff hist -2 m Template:Tool2
- 01:54, 27 June 2022 diff hist +6 m Template:Tool2
- 01:53, 27 June 2022 diff hist 0 Template:Tool2
- 01:53, 27 June 2022 diff hist +78 Template:Tool2 description: {{{{ IF ...}}} , and style smaller italics
- 01:48, 27 June 2022 diff hist -53 Template:StaffInfo DJ remove "phone" "email", make "primary supervisor" span 3 rows
- 01:46, 27 June 2022 diff hist -6 Template:StaffInfo DJ TESTING added "primary" supervisor
- 01:43, 27 June 2022 diff hist +13 DUMMY TOOL
- 01:42, 27 June 2022 diff hist 0 Template:Tool2 move Description, Mfg, Model above supervisors
- 01:40, 27 June 2022 diff hist -68 Template:Tool2 remove table split after supervisors, use HR instead
- 01:38, 27 June 2022 diff hist +18 m Template:Tool2
- 01:37, 27 June 2022 diff hist -86 Template:Tool2 try removing table break, use HR instead
- 01:34, 27 June 2022 diff hist -6 DUMMY TOOL
- 01:30, 27 June 2022 diff hist -28 m Template:Tool2
- 01:28, 27 June 2022 diff hist +27 m Template:Tool2
- 01:27, 27 June 2022 diff hist +1 m Template:Tool2
- 01:27, 27 June 2022 diff hist +18 Template:Tool2 combine super/super2 into one table
- 01:21, 27 June 2022 diff hist -26 Template:Tool2 Undo revision 160044 by John d (talk) Tag: Undo
- 01:20, 27 June 2022 diff hist -1 Template:Tool2 undo revision 157023 by John d (talk)
- 01:18, 27 June 2022 diff hist +1 m Template:Tool2
- 01:17, 27 June 2022 diff hist +26 Template:Tool2 tool info at top, then supervisors, then materials/categories
- 01:13, 27 June 2022 diff hist +131 m Template:StaffInfoSecondary DJ
- 01:12, 27 June 2022 diff hist +2 m Template:StaffInfo DJ
- 01:12, 27 June 2022 diff hist +32 Template:StaffInfo DJ
- 01:11, 27 June 2022 diff hist +1,132 Template:StaffContactInfo DJ updated docs on how to edit contact info
- 01:07, 27 June 2022 diff hist -566 Template:Tool2 updated documentation pointing to Template:StaffContactInfo_DJ
- 00:58, 27 June 2022 diff hist 0 m Template:StaffContactInfo DJ
- 00:58, 27 June 2022 diff hist +133 Template:StaffContactInfo DJ changed all {{{super}}}-->{{{1}}}, and added example sytax
- 00:54, 27 June 2022 diff hist -12 Template:StaffContactInfo DJ changed only Tony and Demis {{{super}}}--> {{{1}}}
- 00:52, 27 June 2022 diff hist +194 Template:StaffContactInfo DJ added includeonly & noinclude sections
- 00:51, 27 June 2022 diff hist +1,761 N Template:StaffContactInfo DJ copied #IFEQ section of "tool2_DJ"
- 00:50, 27 June 2022 diff hist -1,721 Template:Tool2 deleted Staff contact info {{ifeq}}, replaced with {{StaffContactInfo_DJ}}
- 00:40, 27 June 2022 diff hist +116 Template:Tool2
- 00:38, 27 June 2022 diff hist -6 Template:Tool2
- 00:38, 27 June 2022 diff hist -12 Template:StaffInfoSecondary DJ
- 00:34, 27 June 2022 diff hist +39 Template:StaffInfoSecondary DJ
- 00:26, 27 June 2022 diff hist +3 Template:Tool2