User contributions
Jump to navigation
Jump to search
- 12:03, 24 April 2024 diff hist +2 Process Group - Process Control Data Moved litho to the bottom since it's updated less often current Tag: Visual edit: Switched
- 11:48, 24 April 2024 diff hist +94 Nanofab Job Postings moved closed positions to lower section current Tag: Visual edit
- 17:09, 9 April 2024 diff hist +93 ICP Etching Recipes →Through Silicon Via (TSV) etch (DSEiii): no-wax proces sis acceptable Tag: Visual edit
- 17:00, 9 April 2024 diff hist +10 m Stepper 3 (ASML DUV) →Operating Procedures Tag: Visual edit
- 23:06, 4 April 2024 diff hist -31 Step Profilometer (KLA Tencor P-7) updated specs current Tag: Visual edit
- 22:44, 4 April 2024 diff hist -10 m Calculators + Utilities →CAD Files & Templates Tag: Visual edit
- 22:41, 4 April 2024 diff hist +73 N File:Contact-AlignMarks Vernier DemisDJohn v4.oas Contact Alignment Marks redesigned by Demis D. John - OASIS current
- 22:41, 4 April 2024 diff hist +71 N File:Contact-AlignMarks Vernier DemisDJohn v4.gds Contact Alignment Marks redesigned by Demis D. John - GDS current
- 22:37, 4 April 2024 diff hist 0 File:Contact-AlignMarks Vernier DemisDJohn v3 Screenshot.png.png John d uploaded a new version of File:Contact-AlignMarks Vernier DemisDJohn v3 Screenshot.png.png current
- 22:36, 4 April 2024 diff hist +341 m Calculators + Utilities →General CAD files for Litho Tag: Visual edit
- 21:25, 4 April 2024 diff hist +60 m MLA150 - CAD Files and Templates →Alignment Marks current Tag: Visual edit
- 21:22, 4 April 2024 diff hist +1 m Calculators + Utilities →General CAD files for Litho Tag: Visual edit
- 00:00, 4 April 2024 diff hist +193 Calculators + Utilities →General CAD files for Litho: screenshot of Contact-AlignMarks_Vernier_DemisDJohn_v3.oas Tag: Visual edit: Switched
- 23:57, 3 April 2024 diff hist +58 N File:Contact-AlignMarks Vernier DemisDJohn v3 Screenshot.png.png
- 23:53, 3 April 2024 diff hist +34 m Calculators + Utilities →General CAD files for Litho: author credits for contact mark Tag: Visual edit
- 23:53, 3 April 2024 diff hist +78 Calculators + Utilities →General CAD files for Litho: updated contact mark to v3, in OASIS and GDS format Tag: Visual edit
- 23:50, 3 April 2024 diff hist +71 N File:Contact-AlignMarks Vernier DemisDJohn v3.gds Contact Alignment Marks redesigned by Demis D. John - GDS current
- 23:49, 3 April 2024 diff hist +73 N File:Contact-AlignMarks Vernier DemisDJohn v3.oas Contact Alignment Marks redesigned by Demis D. John - OASIS current
- 20:29, 3 April 2024 diff hist +145 Calculators + Utilities →General CAD files for Litho: added contact alignment mark Tag: Visual edit
- 17:09, 1 April 2024 diff hist +806 Nanofab Job Postings added SUmmer '24 etch and dep internsip positions to OPEN positions Tag: Visual edit