Process Control Data are standardized process, run by staff, allowing for day-to-day or year-by-year comparisons of a tool's performance. This is similar (but not identical to) [https://en.wikipedia.org/wiki/Statistical_process_control Statistical Process Control].
  +
 
These are the same links found on individual tool pages, in the '''''Recipes > <<tool page>> > Process Control''''' section.
 
These are the same links found on individual tool pages, in the '''''Recipes > <<tool page>> > Process Control''''' section.
   
  +
__TOC__
= Lithography (Process Control Data) =
 
''Process Control Data for Nanofab Lithography/patterning tools.''
 
   
== [[Stepper_Recipes#Stepper_3_.28ASML_DUV.29|Stepper #3 (ASML DUV)]] ==
 
 
*''The Process Group regularly measures data on lithography Critical Dimension ("CD") and Wafer-stage Particulate Contamination for this tool, using a sensitive lithography process that will reveal small changes in Dose repeatability and wafer flatness.''
 
*[https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=1804752281 '''Plots of CD Repeatability''']
 
*[https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=0 '''Data for CD Uniformity and Particulate Contamination''']
 
 
:{|
 
|[[File:ASML CD Cals - Example Table.jpg|alt=ASML CD Calibration data - Screenshot of Table|none|thumb|300x300px|''Example of Data Table with SEM's of 320nm features. [https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=0 Click for full data table.]''|link=https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=0]]
 
|[[File:ASML CD Cals - Example Plot.jpg|alt=ASML CD Calibration Data - Screenshot of SPC Plot|none|thumb|''Example SPC Chart - Measured Critical Dimension "CD" versus Date. [https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=1804752281 Click for charts.]''|link=https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=1804752281]]
 
|}
 
 
<hr style="height:5px">
 
<hr style="height:5px">
 
   
 
=Deposition (Process Control Data)=
 
=Deposition (Process Control Data)=
Line 104: Line 92:
   
 
*[[Oxford ICP Etcher - Process Control Data|InP Ridge Etch with Cl2/CH4/H2 @ 60°C]] - ''No data prior to 2023-01-20''
 
*[[Oxford ICP Etcher - Process Control Data|InP Ridge Etch with Cl2/CH4/H2 @ 60°C]] - ''No data prior to 2023-01-20''
  +
  +
 
<hr style="height:5px">
 
<hr style="height:5px">
  +
 
=Lithography (Process Control Data)=
 
''Process Control Data for Nanofab Lithography/patterning tools.''
  +
 
==[[Stepper_Recipes#Stepper_3_.28ASML_DUV.29|Stepper #3 (ASML DUV)]]==
  +
 
*''The Process Group regularly measures data on lithography Critical Dimension ("CD") and Wafer-stage Particulate Contamination for this tool, using a sensitive lithography process that will reveal small changes in Dose repeatability and wafer flatness.''
 
*[https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=1804752281 '''Plots of CD Repeatability''']
 
*[https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=0 '''Data for CD Uniformity and Particulate Contamination''']
  +
 
:{|
 
|[[File:ASML CD Cals - Example Table.jpg|alt=ASML CD Calibration data - Screenshot of Table|none|thumb|300x300px|''Example of Data Table with SEM's of 320nm features. [https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=0 Click for full data table.]''|link=https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=0]]
 
|[[File:ASML CD Cals - Example Plot.jpg|alt=ASML CD Calibration Data - Screenshot of SPC Plot|none|thumb|''Example SPC Chart - Measured Critical Dimension "CD" versus Date. [https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=1804752281 Click for charts.]''|link=https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=1804752281]]
 
|}

Latest revision as of 12:03, 24 April 2024

Process Control Data are standardized process, run by staff, allowing for day-to-day or year-by-year comparisons of a tool's performance. This is similar (but not identical to) Statistical Process Control.

These are the same links found on individual tool pages, in the Recipes > <<tool page>> > Process Control section.


Deposition (Process Control Data)

Process Control data for various deposition tools in the lab.

PECVD #1 (PlasmaTherm 790)

PECVD #2 (Advanced Vacuum)

ICP-PECVD (Unaxis VLR Dep)

Ion Beam Sputter Deposition (Veeco Nexus)

Old Data (Pre 2022)

Old data in a different format can be found below:




Etching (Process Control Data)

Process Control data for various dry etching tools in the lab.

PlasmaTherm SLR Fluorine Etcher

OLD Process Control Data

Panasonic ICP #1

Old Process Control Data

Panasonic ICP#2

Old Process Control Data

Unaxis VLR Etch

Oxford PlasmaPro Cobra Etcher

Calibration / Process testing data taken using the "InP Ridge Etch" process: Cl2/CH4/H2 @ 60°C, 1cm piece with ~50% SiO2 hardmask.

Old Process Control Data




Lithography (Process Control Data)

Process Control Data for Nanofab Lithography/patterning tools.

Stepper #3 (ASML DUV)

ASML CD Calibration data - Screenshot of Table
Example of Data Table with SEM's of 320nm features. Click for full data table.
ASML CD Calibration Data - Screenshot of SPC Plot
Example SPC Chart - Measured Critical Dimension "CD" versus Date. Click for charts.