Back to Vacuum Deposition Recipes.
PECVD 1 (PlasmaTherm 790)
SiN deposition (PECVD #1)
- SiN Deposition Recipe
- SIN data
- Low Stress Si3N4 - Variable Stress Recipes
- Low Stress Si3N4 - Variable Stress Plot
SiO2 deposition (PECVD #1)
SiOxNy deposition (PECVD #1)
PECVD 2 (Advanced Vacuum)
SiN deposition (PECVD #2)
SiO2 deposition (PECVD #2)
ICP-PECVD (Unaxis VLR)
SiN deposition (Unaxis VLR)
SiN (2% SiH4)
SiN (2% SiH4 - No-Ar)
50° | 100° | 250° |
---|---|---|
SiN (2% SiH4 - No-Ar - Extra N2)
50° | 100° | 250° |
---|---|---|
SiN (100% SiH4 )
50° | 100° | 250° |
---|---|---|
SiO2 deposition (Unaxis VLR)
SiO2 (2% SiH4)
50° | 100° | 250° |
---|---|---|
SiO2 (2% SiH4 - No Ar)
50° | 100° | 250° |
---|---|---|
SiO2 (100% SiH4 HDR)
50° | 100° | 250° |
---|---|---|
SiO2 (100% SiH4 LDR)
50° | 100° | 250° |
---|---|---|
Amorphous Si (100%SiH4 Ar He)
90° | 250° |
---|---|