Line 153: Line 153:
 
|
 
|
 
*[[Media:PECVD2-SiO2-Recipe-100%SiH4-HDR-100C.pdf|SiO<sub>2</sub> Deposition Recipe - HDR (100°)]]
 
*[[Media:PECVD2-SiO2-Recipe-100%SiH4-HDR-100C.pdf|SiO<sub>2</sub> Deposition Recipe - HDR (100°)]]
  +
*[[Media:PECVD2-SiO2-HDR-100% SiH4.pdf|SiO<sub>2</sub> Comparison Table - HDR (100°)]]
 
|
 
|
*[[Media:PECVD2-SiO2-Recipe-100%SiH4-HDR-250C.pdf|SiO<sub>2</sub> Deposition Recipe - HDR (250°)]]
+
*[[Media:PECVD2-SiO2-Recipe-100%SiH4-HDR-250C.pdf|SiO<sub>2</sub> Deposition Recipe - HDR (250°)]]
  +
*[[Media:PECVD2-SiO2-HDR-100% SiH4.pdf|SiO<sub>2</sub> Comparison Table - HDR (250°)]]
 
|-
 
|-
 
|}
 
|}
  +
 
=== SiO<sub>2</sub> (100% SiH<sub>4</sub> LDR) ===
 
=== SiO<sub>2</sub> (100% SiH<sub>4</sub> LDR) ===
 
{| border="1" class="wikitable" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center;"
 
{| border="1" class="wikitable" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center;"

Revision as of 13:48, 3 October 2012

Back to Vacuum Deposition Recipes.

PECVD 1 (PlasmaTherm 790)

SiN deposition (PECVD #1)

SiO2 deposition (PECVD #1)

PECVD 2 (Advanced Vacuum)

SiN deposition (PECVD #2)

SiO2 deposition (PECVD #2)

ICP-PECVD (Unaxis VLR)

SiN deposition (Unaxis VLR)

SiN (2% SiH4)

50° 100° 250°

SiN (2% SiH4 - No-Ar)

50° 100° 250°

SiN (2% SiH4 - No-Ar - Extra N2)

50° 100° 250°

SiN (100% SiH4 )

50° 100° 250°

SiO2 deposition (Unaxis VLR)

SiO2 (2% SiH4)

50° 100° 250°

SiO2 (2% SiH4 - No Ar)

50° 100° 250°

SiO2 (100% SiH4 HDR)

50° 100° 250°

SiO2 (100% SiH4 LDR)

50° 100° 250°