PECVD1 Recipes
PECVD 1 (PlasmaTherm 790)
SiN deposition (PECVD #1)
- SiN Standard Recipe
- SiN Data July 2014
- SiN 1000A Thickness uniformity 2014
- Low Stress Si3N4 - Variable Stress Recipes
- Low Stress Si3N4 - Variable Stress Plot
- Deposition rate~11.30nm/min (users must calibrate this prior to critical deps)
- HF e.r.~89nm/min
- Stress~466MPa
- Refractive Index~1.937
SiO2 deposition (PECVD #1)
- Deposition rate~35.73nm/min (users must calibrate this prior to critical deps)
- HF e.r.~610nm/min
- Stress~-402MPa
- Refractive Index~1.460