=[[CAIBE (Oxford Ion Mill)]]= |
=[[CAIBE (Oxford Ion Mill)]]= |
||
*[[media:42-Etching_Platinum_using_Oxford_Ion_Mill_Tool-a.pdf|Pt Etch Recipe]] |
*[[media:42-Etching_Platinum_using_Oxford_Ion_Mill_Tool-a.pdf|Pt Etch Recipe]] |
||
− | *[[media:|Au Etch Recipe]] |
+ | *[[media:44-Etching_Gold_with_Al2O3_Mask_using_Oxford_Ion_Mill_Tool.pdf|Au Etch Recipe]] |