Difference between revisions of "NanoFab Process Group"
Jump to navigation
Jump to search
(created page, Links to various dicing procedures. Added Process Control links as well.) |
(Text replacement - "/wiki/index.php" to "/w/index.php") |
||
(4 intermediate revisions by 2 users not shown) | |||
Line 1: | Line 1: | ||
− | ''This page lists various processes used internally by the [https:// |
+ | ''This page lists various processes used internally by the [https://wiki.nanotech.ucsb.edu/w/index.php?title=Staff_List#Process_Group NanoFab Process Group].'' |
== Dicing Procedures == |
== Dicing Procedures == |
||
Line 6: | Line 6: | ||
* [[ProcessGroup: PR Spin for Dicing Protect - UV6|PR Spin for Dicing Protect]] - ~800nm thick PR only (UV6) |
* [[ProcessGroup: PR Spin for Dicing Protect - UV6|PR Spin for Dicing Protect]] - ~800nm thick PR only (UV6) |
||
* [[ProcessGroup: PR Clean of UV-6|PR Clean of UV-6]] |
* [[ProcessGroup: PR Clean of UV-6|PR Clean of UV-6]] |
||
− | * [[ProcessGroup: Shipping on |
+ | * [[ProcessGroup: Shipping Samples on Dicing Tape+Frame|Shipping Samples on Dicing Tape+Frame]] |
=== Dicing Alignment Mark Exposure === |
=== Dicing Alignment Mark Exposure === |
||
Line 26: | Line 26: | ||
* [[ProcessGroup: Unaxis PM3 Process Verification Procedure|Unaxis PM3: Process Verification Procedure]] |
* [[ProcessGroup: Unaxis PM3 Process Verification Procedure|Unaxis PM3: Process Verification Procedure]] |
||
* [[ProcessGroup: IBD Process Verification Procedure|Veeco IBD: Process Verification Procedure]] |
* [[ProcessGroup: IBD Process Verification Procedure|Veeco IBD: Process Verification Procedure]] |
||
+ | |||
+ | == Equipment Calibration Procedures == |
||
+ | |||
+ | === Lithography Tools === |
||
+ | * [[ProcessGroup: GCA 6300 Stepper|GCA 6300 Stepper #1: Calibration Procedure]] |
||
+ | * [[ProcessGroup: GCA AutoStep 200, Stepper|GCA AutoStep 200, Stepper #2: Calibration procedure]] |
||
+ | * [[ProcessGroup: ASML 5500 Stepper|ASML 5500 Stepper#3: Calibration Verification/Update procedure]] |
Revision as of 12:51, 4 September 2021
This page lists various processes used internally by the NanoFab Process Group.
Dicing Procedures
Photoresist Application, Cleaning and Shipping
- PR Spin for Dicing Protect - ~800nm thick PR only (UV6)
- PR Clean of UV-6
- Shipping Samples on Dicing Tape+Frame
Dicing Alignment Mark Exposure
For providing alignment marks to use while dicing.
- ASML Stepper #3: Dicing Alignment Guides
- How to program the ASML to shoot some alignment markers for use during dicing.
Process Control Calibration Procedures
Etching Tools
- Unaxis PM1: Indium Phosphide Etch Verification Procedure
- ICP#1/2: SiO2 Etch Verification Procedure
- PlasmaTherm SLR: SiO2 Etch Verification Procedure
- PlasmaTherm DSEiii: Si Etch Verification Procedure
Deposition Tools
- PECVD#1: Process Verification Procedure
- PECVD#2: Process Verification Procedure
- Unaxis PM3: Process Verification Procedure
- Veeco IBD: Process Verification Procedure