Difference between revisions of "KLA Tencor P7 - Saving Profile Data"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
m (minor newline fix)
m (newlines fix)
Line 1: Line 1:
 
''To save or export raw numeric data of a profile/scan.''
 
''To save or export raw numeric data of a profile/scan.''
# Click the "APEX" Analysis button to load the profile data in the APEX software. [[File:KLA-Tencor P7 - Saving Data - 1-APEX button.jpg|255x255px]]
+
# Click the "APEX" Analysis button to load the profile data in the APEX software. [[File:KLA-Tencor P7 - Saving Data - 1-APEX button.jpg|255x255px]]
# Press Alt-Tab (maybe multiple times) to Switch to the APEX software, which launches in the background. [[File:KLA-Tencor P7 - Saving Data - 2-switch to APEX.jpg|288x288px]]
+
# Press Alt-Tab (maybe multiple times) to Switch to the APEX software, which launches in the background. [[File:KLA-Tencor P7 - Saving Data - 2-switch to APEX.jpg|288x288px]]
# Go to the '''''Studiables''''' tab, and click "'''''Save the Profile'''''" [[File:KLA-Tencor P7 - Saving Data - 3-Apex Save the Studiable profile.jpg|286x286px]]
+
# Go to the '''''Studiables''''' tab, and click "'''''Save the Profile'''''" [[File:KLA-Tencor P7 - Saving Data - 3-Apex Save the Studiable profile.jpg|286x286px]]
# Save as file type "TXT - ASCII" [[File:KLA-Tencor P7 - Saving Data - 4-Save as TXT.jpg|391x391px]]
+
# Save as file type "TXT - ASCII" [[File:KLA-Tencor P7 - Saving Data - 4-Save as TXT.jpg|391x391px]]
# Choose your data options, typical parameters below: [[File:5-Export Options.jpg|441x441px]]
+
# Choose your data options, typical parameters below: [[File:5-Export Options.jpg|441x441px]]

Revision as of 22:35, 10 April 2019

To save or export raw numeric data of a profile/scan.

  1. Click the "APEX" Analysis button to load the profile data in the APEX software. KLA-Tencor P7 - Saving Data - 1-APEX button.jpg
  2. Press Alt-Tab (maybe multiple times) to Switch to the APEX software, which launches in the background. KLA-Tencor P7 - Saving Data - 2-switch to APEX.jpg
  3. Go to the Studiables tab, and click "Save the Profile" KLA-Tencor P7 - Saving Data - 3-Apex Save the Studiable profile.jpg
  4. Save as file type "TXT - ASCII" KLA-Tencor P7 - Saving Data - 4-Save as TXT.jpg
  5. Choose your data options, typical parameters below: 5-Export Options.jpg