ICP Etching Recipes
Revision as of 16:42, 24 October 2013 by Thibeault (talk | contribs) (→Sapphire Etch (Panasonic 1))
Back to Dry Etching Recipes.
Si Deep RIE (PlasmaTherm/Bosch Etch)
Single-step Si Etching (not Bosch Process!) (Si Deep RIE)
ICP Etch 1 (Panasonic E626I)
SiO2 Etching (Panasonic 1)
SiNx Etching (Panasonic 1)
Al Etch (Panasonic 1)
Cr Etch (Panasonic 1)
Ti Etch (Panasonic 1)
W-TiW Etch (Panasonic 1)
GaAs-AlGaAs Etch (Panasonic 1)
- GaAs-Nanoscale Etch Recipe - PR mask - Cl2-BCl3-Ar
- AlGaAs Etch Recipes - Cl2N2
- GaAs DRIE via Etch Recipes - Cl2-BCl3-Ar PR passivation
GaN Etch (Panasonic 1)
SiC Etch (Panasonic 1)
Sapphire Etch (Panasonic 1)
ICP Etch 2 (Panasonic E640)
SiO2 Etching (Panasonic 2)
SiNx Etching (Panasonic 2)
Al Etch (Panasonic 2)
GaAs Etch (Panasonic 2)
ICP-Etch (Unaxis VLR)
GaAs-AlGaAs Etch (Unaxis VLR)
InP-InGaAs-InAlAs Etch (Unaxis VLR)
- InP Etch Recipe (Cl2N2Ar 200C)
- InP-based Material Etch Profile (Cl2N2Ar200C)
- Unaxis InP Etch Recipe (Cl2H2 Ar 200C) Parameters
- InP-InGaAs Etch Profile (Cl2H2 Ar 200C)