Difference between revisions of "ICP Etching Recipes"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Line 3: Line 3:
 
==SiO<sub>2</sub> Vertical Etch (Panasonic 1)==
 
==SiO<sub>2</sub> Vertical Etch (Panasonic 1)==
 
*[[media:Panasonic1-SiO-Etch.pdf|SiO<sub>2</sub> Vertical Etch Recipe]]
 
*[[media:Panasonic1-SiO-Etch.pdf|SiO<sub>2</sub> Vertical Etch Recipe]]
*[[media:Panasonic1-SiO-Etch-SEM.pdf|SiO<sub>2</sub> SEM image Vertical Etch ]]
+
*[[media:Panasonic1-SiO-Etch-SEM.pdf|SiO<sub>2</sub> Vertical Etch SEM ]]
  
 
==Cr Etch (Panasonic 1)==
 
==Cr Etch (Panasonic 1)==

Revision as of 09:46, 21 August 2013