Difference between revisions of "Direct-Write Lithography Recipes"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
m
m (link to tool page)
Line 4: Line 4:
 
__TOC__
 
__TOC__
  
== Heidelberg Instruments MLA150 ==
+
== [[Maskless Aligner (Heidelberg MLA150)]] ==
 
Photolithography Recipes for the [[Maskless Aligner (Heidelberg MLA150)|Heidelberg MLA150]].  ''Description of litho params- different lasers available, greyscale etc.''
 
Photolithography Recipes for the [[Maskless Aligner (Heidelberg MLA150)|Heidelberg MLA150]].  ''Description of litho params- different lasers available, greyscale etc.''
  

Revision as of 22:32, 13 September 2020

UnderConstruction.jpg

Work In Progress

This article is still under construction. It may contain factual errors. Content is subject to change.


Maskless Aligner (Heidelberg MLA150)

Photolithography Recipes for the Heidelberg MLA150. Description of litho params- different lasers available, greyscale etc.

Positive Resist (MLA150)

General notes: Hotplates used, filters, laser wavelengths, etc.

Resist Spin Cond. Bake Thickness Exposure Time Focus Offset PEB Developer Developer Time Comments
SPR955CM0.9 3 krpm/30” 95°C/60” ~ 0.9 um AZ300MIF

Negative Resist (MLA150)

General notes: Hotplates used, filters, laser wavelengths, etc.

Resist Spin Cond. Bake Thickness Exposure Time Focus Offset PEB Flood Developer Developer Time Comments
AZ5214 6 krpm/30” 95°C/60” ~ 1.0 um 60" AZ300MIF 60"
  • ???