Atomic Layer Deposition Recipes
Revision as of 17:32, 4 July 2013 by Prezioso m (talk | contribs)
The printable version is no longer supported and may have rendering errors. Please update your browser bookmarks and please use the default browser print function instead.
Back to Vacuum Deposition Recipes.
Atomic Layer Deposition (Oxford FlexAL)
Al2O3 deposition (ALD)
AlN deposition (ALD)
HfO2 deposition (ALD)
SiO2 deposition (ALD)
ZrO2 deposition (ALD)
TiO2 deposition (ALD)
TiO2 recipe WJM_TDMAT_H2O_r2 water dose 1s, at 200C, gives grow rate 0.11 nm/cy (pdf file to be added)