Difference between revisions of "Dicing Saw (ADT)"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
(→‎Operating Procedures: added "initial setup before cutting" link)
(New SOP rev)
 
(24 intermediate revisions by 4 users not shown)
Line 1: Line 1:
{{tool|{{PAGENAME}}
+
{{tool2|{{PAGENAME}}
 
|picture=ADT.jpg
 
|picture=ADT.jpg
 
|type = Packaging
 
|type = Packaging
|super= Aidan Hopkins
+
|super= Lee Sawyer
  +
|super2= Aidan Hopkins
|phone= 805-893-3918x208
 
|location=Dicing Saw Room
+
|location=Backend Lab: ESB 1111
|email=hopkins@ece.ucsb.edu
 
 
|description = ADT Dicing Saw
 
|description = ADT Dicing Saw
  +
|model = ADT 7100
 
|manufacturer = Advanced Dicing Technologies Ltd.
 
|manufacturer = Advanced Dicing Technologies Ltd.
 
|materials =
 
|materials =
 
|toolid=49
 
|toolid=49
 
}}
 
}}
== About ==
+
==About==
  +
The Model 7100 Series is a semi-automatic dicing saw. Semiconductor, glass, and plastic substrates of all types can be automatically or manually cut. This dicing Saw is optimized for multi-angle dicing of tight tolerance substrates up to 200 mm diameter in size.
The ADT 7100 Dicing Saw is optimized for multi-angle dicing of thin, tight tolerance products up to 200 mm x 200 mm. It is currently setup for dicing up to 8” diameter wafers. Check the Dicing Saw Recipes page for the blades we currently stock.
 
   
 
Check the [https://wiki.nanotech.ucsb.edu/w/index.php?title=Packaging_Recipes#Dicing_Saw_Recipes_.28ADT_7100.29 Dicing Saw Recipes page] for the blades we currently stock.
== Detailed Specifications ==
 
   
  +
An ADT WM-966 tape applicator is used to mount samples to UV-release tape for dicing and an Ultron Systems UH104-8 UV lamp system is used to release samples post dicing.
== Operating Procedures ==
 
* [[ADT 7100 - Initial Setup Before Cutting|Setting up the Saw before Cutting]]
 
* [[ADT 7100 - Standard Dicing Procedure - Programmed Cut Map|Standard Dicing Procedure - Programmed Cut Map]]
 
* [[ADT 7100 - Standard Dicing Procedure - Single Cuts|Standard Dicing Procedure - Single Cuts]]
 
   
  +
Contact Staff for blades and dicing frames for your group.
==== [[Recipe Recovery Procedure]] ====
 
# [[File:Image.png]]Click on the Programming Workspace
 
# Go to any recipe
 
# Click 'Recipe Import'[[File:Recipe import.png]]
 
# Select 'd: [New Volume]' from 'Folder List'[[File:Volume d.jpg|533x533px]]
 
# Open folder 'ADT'. Open Folder 'ADT-7100-8544150816'. Open folder 'db'. Open folder 'exports'
 
# Find you recipe in the box to the right and double click on it
 
# Verify group name is correct under 'Recipe Info'
 
# Click 'OK'
 
# Click 'Replace'
 
# Repeat for additional recipes
 
   
 
==Detailed Specifications==
== Recipes ==
 
  +
* Packaging Recipes > [https://www.nanotech.ucsb.edu/wiki/index.php/Packaging_Recipes?venotify=created#Dicing_Saw_Recipes_.28ADT_7100.29 Dicing Saw Recipes (ADT 7100)]
 
  +
*Maximum Wafer Size: 8"
Be sure to also see the methods for protecting your sample from dicing dust, and mounting/unmounting.
 
  +
*Parts mounted to UV-release tape for dicing
  +
*Automated cut maps at multiple angles (0° and 90° typical)
  +
*~Few micron alignment to on-wafer features.
  +
*Thermocarbon Resnoid dicing blades provided by Staff
  +
 
==Operating Procedures==
  +
  +
*[https://wiki.nanofab.ucsb.edu/w/images/5/54/ADT_SOP_Rev_J.pdf ADT Dicing Saw Standard Operating Procedure]
  +
*[https://wiki.nanotech.ucsb.edu/w/images/0/01/Tape_Station_SOP_Rev_A.pdf Tape Station Standard Operating Procedure]
  +
*[https://wiki.nanofab.ucsb.edu/w/images/5/5a/Ultron_1042R_Film_specs.pdf Ultron Systems, Inc. 1042R Anti-Static Ultraviolet Film TDS]
  +
*[[ADT 7100 - Recovering an Old Recipe (2019)|Recovering an Old Recipe]]
  +
  +
 
==Recipes==
  +
  +
*Recipes > Packaging > '''[[Packaging Recipes#Dicing Saw Recipes .28ADT 7100.29|Dicing Saw Recipes (ADT 7100)]]'''
  +
 
Be sure to also see the recipes for protecting your sample from dicing dust, and mounting/unmounting.

Latest revision as of 15:11, 17 October 2023

Dicing Saw (ADT)
ADT.jpg
Location Backend Lab: ESB 1111
Tool Type Packaging
Manufacturer Advanced Dicing Technologies Ltd.
Model ADT 7100
Description ADT Dicing Saw

Primary Supervisor Lee Sawyer
(805) 893-2123
lee_sawyer@ucsb.edu

Secondary Supervisor

Aidan Hopkins


Recipes

SignupMonkey: Sign up for this tool


About

The Model 7100 Series is a semi-automatic dicing saw. Semiconductor, glass, and plastic substrates of all types can be automatically or manually cut. This dicing Saw is optimized for multi-angle dicing of tight tolerance substrates up to 200 mm diameter in size.

Check the Dicing Saw Recipes page for the blades we currently stock.

An ADT WM-966 tape applicator is used to mount samples to UV-release tape for dicing and an Ultron Systems UH104-8 UV lamp system is used to release samples post dicing.

Contact Staff for blades and dicing frames for your group.

Detailed Specifications

  • Maximum Wafer Size: 8"
  • Parts mounted to UV-release tape for dicing
  • Automated cut maps at multiple angles (0° and 90° typical)
  • ~Few micron alignment to on-wafer features.
  • Thermocarbon Resnoid dicing blades provided by Staff

Operating Procedures


Recipes

Be sure to also see the recipes for protecting your sample from dicing dust, and mounting/unmounting.