Difference between revisions of "PECVD1 Recipes"
Jump to navigation
Jump to search
Line 14: | Line 14: | ||
== Other recipes (PECVD1)== |
== Other recipes (PECVD1)== |
||
+ | * [[media:PECVD1-SiON-Recipe.pdf|Low Stress Si<sub>3</sub>N<sub>4</sub> - Variable Stress Recipes]] |
||
+ | * [[media:PECVD1-SiON-Recipe.pdf|Low Stress Si<sub>3</sub>N<sub>4</sub> - Variable Stress Plot]] |
||
+ | |||
== LS SiO<sub>x</sub>N<sub>y</sub> deposition (PECVD #1) == |
== LS SiO<sub>x</sub>N<sub>y</sub> deposition (PECVD #1) == |
||
<!-- Placeholders - Not uploaded yet--> |
<!-- Placeholders - Not uploaded yet--> |
Revision as of 09:55, 10 December 2014
PECVD 1 (PlasmaTherm 790)
SiN deposition (PECVD #1)
- SiN Standard Recipe
- SiN Data 2014
- SiN 1000A Thickness uniformity 2014
- Low Stress Si3N4 - Variable Stress Recipes
- Low Stress Si3N4 - Variable Stress Plot
SiO2 deposition (PECVD #1)
Other recipes (PECVD1)
LS SiOxNy deposition (PECVD #1)
- SiOxNy Deposition Recipes - Varying N/O Ratio
- SiOxNy Stress/Index vs. O/N Ratio
- SiOxNy Recipe
- SiOxNy Data December 2014
- SiOxNy 3000A Thickness uniformity 2014