Difference between revisions of "RIE Etching Recipes"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Line 6: Line 6:
   
 
=[[RIE 3 (MRC)]] =
 
=[[RIE 3 (MRC)]] =
==InP-InGaAsP-InGaAlAs Etching (RIE 5)==
 
*[[media:RIE2-InGaAs-InP-InAlAs-Etch-Plasma-RIE-RevA.pdf|InP-InGaAsP-InAlGaAs Etch Recipes - CH<sub>4</sub>-H<sub>2</sub>-Ar]]
 
   
 
=[[RIE 5 (PlasmaTherm)]] =
 
=[[RIE 5 (PlasmaTherm)]] =

Revision as of 16:40, 23 October 2013