Difference between revisions of "Holographic Lith/PL Setup (Custom)"
Jump to navigation
Jump to search
(Created page with "{{tool|{{PAGENAME}} |picture=Holograph.jpg |type = Lithography |super= Ning Cao |phone=(805) 839-5689 |location=Bay 6 |email=Ningcao@ece.ucsb.edu |description = Custom Built Int…") |
|||
(One intermediate revision by the same user not shown) | |||
Line 8: | Line 8: | ||
|description = Custom Built Interference Lithography |
|description = Custom Built Interference Lithography |
||
|manufacturer = Kimmon |
|manufacturer = Kimmon |
||
+ | |toolid=35 |
||
}} |
}} |
||
= About = |
= About = |
Revision as of 06:56, 11 July 2012
|
About
The interference lithography system at UCSB uses a 15mW, single-mode, 325 nm HeCd laser that is filtered and expanded by pinhole filters to produce the large area exposure beam. The system uses a simple mirror configuration with a fixed 90 degree angle between the mirror and sample. The entire mirror/sample assembly is rotated in 0.1 degree increments to change the grating pitch from ~ 200 nm to ~ 280 nm (35 to 55 degrees) over an ~ 2 cm x 2 cm exposure area. SPR3001 resist spin-coated to ~ 80 nm thickness is used for grating exposure. 2-D gratings can be formed by rotating the sample and doing multiple exposures. Total exposure times are controlled by a manual shutter and are generally several minutes in length.
Detailed Specifications
- 15 mW single TEM mode HeCd laser
- ~ 2 cm x 2 cm uniform exposure area
- ~ several minute exposure times
- Grating period adjustable from ~200 to ~280 nm with a single stage