File:FL-ICP Process Control Data Example.jpg
Jump to navigation
Jump to search
Size of this preview: 800 × 475 pixels. Other resolutions: 320 × 190 pixels | 1,102 × 654 pixels.
Original file (1,102 × 654 pixels, file size: 138 KB, MIME type: image/jpeg)
Example plot of Fluorine ICP Etcher - Process Control Data
File history
Click on a date/time to view the file as it appeared at that time.
Date/Time | Thumbnail | Dimensions | User | Comment | |
---|---|---|---|---|---|
current | 12:06, 20 January 2023 | 1,102 × 654 (138 KB) | John d (talk | contribs) |