File:Au oxidation by O2-N2 ash.jpg
Jump to navigation
Jump to search
Size of this preview: 800 × 402 pixels. Other resolutions: 320 × 161 pixels | 1,388 × 697 pixels.
Original file (1,388 × 697 pixels, file size: 124 KB, MIME type: image/jpeg)
In high oxidation environment, in this case by O2/N2 mixture recipe, gold surface can oxidize as shown by the XPS data.