Pressure drop indicates completion of etch. Once pressure flattens etching is complete. |
Pressure drop indicates completion of etch. Once pressure flattens etching is complete. |
||
− | [[File:YES-SPR220vsTemp.jpg|578x578px]] |
+ | [[File:YES-SPR220vsTemp.jpg|578x578px]]<br /> |
− | [[File:PPR 220-7 Etch Rates vs Temperature.jpg|left|thumb|572x572px|alt=|Oxygen only recipes, 3KW power, O2 2000sccm]] |
||
− | <br /> |