Pressure drop indicates completion of etch. Once pressure flattens etching is complete. 
+
Pressure drop indicates completion of etch.  
  
[[File:YES150CResists.jpg]]
+
Once pressure flattens etching is complete. 
 +
 
 +
There is uncertainty in the exact completion time, somewhere between the peak pressure and the point where it goes flat.  Using known PR thicknesses you can estimate etch rate from these plots. 
 +
 
 +