Difference between revisions of "Vacuum Deposition Recipes"
Jump to navigation
Jump to search
(minor link edit sputter5) |
(sputt4 link to TiN - recipes table) |
||
Line 799: | Line 799: | ||
| [[Sputtering Recipes|A]] |
| [[Sputtering Recipes|A]] |
||
| <br> |
| <br> |
||
+ | | [https://www.nanotech.ucsb.edu/wiki/index.php/Sputtering_Recipes#Sputter_4_.28AJA_ATC_2200-V.29 R] |
||
− | | [[Sputtering Recipes|R]] |
||
| <br> |
| <br> |
||
| [[Sputtering_Recipes#Ion_Beam_Deposition_.28Veeco_NEXUS.29|A]] |
| [[Sputtering_Recipes#Ion_Beam_Deposition_.28Veeco_NEXUS.29|A]] |
Revision as of 09:09, 9 July 2018
- R = Recipe is available. Clicking this link will take you to the recipe.
- A = Material is available for use, but no recipes are provided.