| width="65" bgcolor="#daf1ff" | [[Sputtering Recipes#Sputter_1_.28Custom.29|Sputter 1 (Custom)]] | | width="65" bgcolor="#daf1ff" | [[Sputtering Recipes#Sputter_1_.28Custom.29|Sputter 1 (Custom)]] | ||
| width="65" bgcolor="#daf1ff" | [[Sputtering Recipes#Sputter_2_.28SFI_Endeavor.29|Sputter 2<br>(SFI Endeavor)]] | | width="65" bgcolor="#daf1ff" | [[Sputtering Recipes#Sputter_2_.28SFI_Endeavor.29|Sputter 2<br>(SFI Endeavor)]] | ||
− | | width="65" bgcolor="#daf1ff" | [[Sputtering_Recipes#Sputter_3_.28AJA_ATC_2000-F.29|Sputter 3<br>(ATC 2000-F)]] | + | | width="65" bgcolor="#daf1ff" | [[Sputtering_Recipes#Sputter_3_.28AJA_ATC_2000-F.29|Sputter 3<br>(AJA ATC 2000-F)]] |
− | | width="65" bgcolor="#daf1ff" | [[Sputtering_Recipes#Sputter_4_.28AJA_ATC_2200-V.29|Sputter 4<br>(ATC 2200-V)]] | + | | width="65" bgcolor="#daf1ff" | [[Sputtering_Recipes#Sputter_4_.28AJA_ATC_2200-V.29|Sputter 4<br>(AJA ATC 2200-V)]] |
| width="65" bgcolor="#daf1ff" | [[Sputter 5 (AJA ATC 2200-V)]] | | width="65" bgcolor="#daf1ff" | [[Sputter 5 (AJA ATC 2200-V)]] | ||
| width="55" bgcolor="#daf1ff" | [[Sputtering_Recipes#Ion_Beam_Deposition_.28Veeco_NEXUS.29|Ion Beam<br>Deposition (Veeco Nexus)]] | | width="55" bgcolor="#daf1ff" | [[Sputtering_Recipes#Ion_Beam_Deposition_.28Veeco_NEXUS.29|Ion Beam<br>Deposition (Veeco Nexus)]] |
Revision as of 14:12, 1 May 2018
- R = Recipe is available. Clicking this link will take you to the recipe.
- A = Material is available for use, but no recipes are provided.