Difference between revisions of "Template:Publications"
(updated notes to show how to make new post) |
(added Warren's paper) |
||
(One intermediate revision by the same user not shown) | |||
Line 9: | Line 9: | ||
<!------------- Select Publications ----------------> |
<!------------- Select Publications ----------------> |
||
+ | == [https://doi.org/10.1364/OL.394121 Deuterated silicon dioxide for heterogeneous integration of ultra-low-loss waveguides] == |
||
+ | Warren Jin, Demis D. John, Jared F. Bauters, Tony Bosch, Brian J. Thibeault, and John E. Bowers |
||
+ | |||
+ | [https://doi.org/10.1364/OL.394121 Optics Letters Vol. 45, Issue 12, pp. 3340-3343 (2020)] |
||
== [https://www.nature.com/articles/s41586-019-1666-5 Quantum supremacy using a programmable superconducting processor] == |
== [https://www.nature.com/articles/s41586-019-1666-5 Quantum supremacy using a programmable superconducting processor] == |
||
Line 15: | Line 19: | ||
[https://www.nature.com/articles/s41586-019-1666-5 Nature, volume 574, pages 505–510 (2019)] |
[https://www.nature.com/articles/s41586-019-1666-5 Nature, volume 574, pages 505–510 (2019)] |
||
− | == An optical-frequency synthesizer using integrated photonics == |
+ | == [https://www.nature.com/articles/s41586-018-0065-7 An optical-frequency synthesizer using integrated photonics] == |
D. T. Spencer, T. Drake, ... John E. Bowers, Scott A. Diddams, Scott B. Papp |
D. T. Spencer, T. Drake, ... John E. Bowers, Scott A. Diddams, Scott B. Papp |
||
[https://www.nature.com/articles/s41586-018-0065-7 Nature, volume 557, pages 81–85 (2018)] |
[https://www.nature.com/articles/s41586-018-0065-7 Nature, volume 557, pages 81–85 (2018)] |
||
− | == Continuous-wave operation of m-plane GaN-based vertical-cavity surface-emitting lasers with a tunnel junction intracavity contact == |
+ | == [https://aip.scitation.org/doi/10.1063/1.5007746 Continuous-wave operation of m-plane GaN-based vertical-cavity surface-emitting lasers with a tunnel junction intracavity contact] == |
C.A. Forman, S.G. Lee, ... S.P. DenBaars, S. Nakamura |
C.A. Forman, S.G. Lee, ... S.P. DenBaars, S. Nakamura |
||
[https://aip.scitation.org/doi/10.1063/1.5007746 Applied Physics Letters, Vol. 112, Issue 11, 2018] |
[https://aip.scitation.org/doi/10.1063/1.5007746 Applied Physics Letters, Vol. 112, Issue 11, 2018] |
||
− | == DARKNESS: A Microwave Kinetic Inductance Detector Integral Field Spectrograph for High-contrast Astronomy == |
+ | == [https://iopscience.iop.org/article/10.1088/1538-3873/aab5e7/meta DARKNESS: A Microwave Kinetic Inductance Detector Integral Field Spectrograph for High-contrast Astronomy] == |
S.R. Meeker, B.A. Mazin, ... G. Vasisht, E. Serabyn |
S.R. Meeker, B.A. Mazin, ... G. Vasisht, E. Serabyn |
||
[https://iopscience.iop.org/article/10.1088/1538-3873/aab5e7/meta Astronomical Society of the Pacific, Volume 130, Issue 988, pp. 065001 (2018)] |
[https://iopscience.iop.org/article/10.1088/1538-3873/aab5e7/meta Astronomical Society of the Pacific, Volume 130, Issue 988, pp. 065001 (2018)] |
||
− | == Dielectrophoretic Nanoparticle Aggregation for On-Demand Surface Enhanced Raman Spectroscopy Analysis == |
+ | == [https://doi.org/10.1021/acs.analchem.8b00510 Dielectrophoretic Nanoparticle Aggregation for On-Demand Surface Enhanced Raman Spectroscopy Analysis] == |
R. Salemmilani, B.D. Piorek, A.W. Fountain, M. Moskovits, C.D. Meinhart |
R. Salemmilani, B.D. Piorek, A.W. Fountain, M. Moskovits, C.D. Meinhart |
||
[https://doi.org/10.1021/acs.analchem.8b00510 Analytical Chemistry, 90, 13, 7930-7936 (2018)] |
[https://doi.org/10.1021/acs.analchem.8b00510 Analytical Chemistry, 90, 13, 7930-7936 (2018)] |
||
− | == Demonstration of Constant 8 W/mm Power Density at 10, 30, and 94 GHz in State-of-the-Art Millimeter-Wave N-Polar GaN MISHEMTs == |
+ | == [https://doi.org/10.1109/TED.2017.2770087 Demonstration of Constant 8 W/mm Power Density at 10, 30, and 94 GHz in State-of-the-Art Millimeter-Wave N-Polar GaN MISHEMTs] == |
B. Romanczyk, S. Wienecke, M. Guidry, H. Li, E. Ahmadi, X. Zheng, S. Keller, U.K. Mishra |
B. Romanczyk, S. Wienecke, M. Guidry, H. Li, E. Ahmadi, X. Zheng, S. Keller, U.K. Mishra |
||
Revision as of 19:22, 20 July 2020
Publications using the Nanofab
Deuterated silicon dioxide for heterogeneous integration of ultra-low-loss waveguides
Warren Jin, Demis D. John, Jared F. Bauters, Tony Bosch, Brian J. Thibeault, and John E. Bowers
Optics Letters Vol. 45, Issue 12, pp. 3340-3343 (2020)
Quantum supremacy using a programmable superconducting processor
F. Arute, K. Arya, ... Harmut Neven, John M. Martinis
Nature, volume 574, pages 505–510 (2019)
An optical-frequency synthesizer using integrated photonics
D. T. Spencer, T. Drake, ... John E. Bowers, Scott A. Diddams, Scott B. Papp
Nature, volume 557, pages 81–85 (2018)
Continuous-wave operation of m-plane GaN-based vertical-cavity surface-emitting lasers with a tunnel junction intracavity contact
C.A. Forman, S.G. Lee, ... S.P. DenBaars, S. Nakamura
Applied Physics Letters, Vol. 112, Issue 11, 2018
DARKNESS: A Microwave Kinetic Inductance Detector Integral Field Spectrograph for High-contrast Astronomy
S.R. Meeker, B.A. Mazin, ... G. Vasisht, E. Serabyn
Astronomical Society of the Pacific, Volume 130, Issue 988, pp. 065001 (2018)
Dielectrophoretic Nanoparticle Aggregation for On-Demand Surface Enhanced Raman Spectroscopy Analysis
R. Salemmilani, B.D. Piorek, A.W. Fountain, M. Moskovits, C.D. Meinhart
Analytical Chemistry, 90, 13, 7930-7936 (2018)
Demonstration of Constant 8 W/mm Power Density at 10, 30, and 94 GHz in State-of-the-Art Millimeter-Wave N-Polar GaN MISHEMTs
B. Romanczyk, S. Wienecke, M. Guidry, H. Li, E. Ahmadi, X. Zheng, S. Keller, U.K. Mishra
IEEE Transactions On Electron Devices, Vol. 65, No. 1 (2018)