Stocked Chemical List
Jump to navigation
Jump to search
The printable version is no longer supported and may have rendering errors. Please update your browser bookmarks and please use the default browser print function instead.
You can sort the following table using the ↑ / ↓ buttons in the title row. Your browser's "Find" ⌘-F function also works.
CHEMICAL | DESCRIPTION | VENDOR | Other Names/Notes |
---|---|---|---|
Acetone, 4L, 4 bt = 1 cs | ACETONE ACS SAFE-COTE 4L Percent Purity ≥99.5% | FISHER SCIENTIFIC | ACE |
Propanol, 4L, 4 bt = 1 cs | 2-PROPANOL OPTIM AGRADE Percent Purity ≥99.9% | FISHER SCIENTIFIC | ISO, IPA, Isopropanol |
Ethanol | DEHYDRATED ALCOHOL, 200 PROOF, UNDENATURED, USP GRADE- 4LGLASS | SPECTRUM CHEMICALS & LAB | |
Methanol, 4L, 4 bt = 1 cs | METHANOL OPTIMA GRADE 4L Percent Purity ≥99.9% | FISHER SCIENTIFIC | |
Toluene, 4 L | TOLUENE OPTIMA GRADE 4L Percent Purity ≥99.8% | FISHER SCIENTIFIC | |
Ethylene Glycol | ETHYLENE GLYCOL LABORATORY GRADE | FISHER SCIENTIFIC | |
Amyl Acetate, 4L bottle | AMYL ACETATE LABORATORY GRADE 4L | FISHER SCIENTIFIC | |
MIBK, 4L bottle | Methyl iso-Butyl Ketone (Certified ACS), Grade Certified ACS Reagent | FISHER SCIENTIFIC | |
Chloroform, 2.5 L | Chloroform, 99+%, Acros Organics | FISHER SCIENTIFIC | |
Xylenes, 1 liter | XYLENES ACS 4L Percent Purity ≥98.5% | FISHER SCIENTIFIC | |
T1100 BCB rinse solvent | RINSE T1100 4 LITER GLASS BOTTLE | MICROCHEM CORP. | |
Nitric, 500ml. | NITRIC ACID IND SAFECOTE 2,5L, Assay Percent Range 70% | FISHER SCIENTIFIC | |
Sulfuric, 2.5 L | SULFURIC AC 21/2L IND SAFECOTE Assay Percent Range 95.0 to 98.0 w/w % | FISHER SCIENTIFIC | H2SO4 |
O-Phosphoric, 2.5 L | O-PHOSPHORIC ACID Percent Purity ≥85.0% (w/w) | FISHER SCIENTIFIC | H3PO4 |
Citric acid, liquid, 1.0 M, 1L | CITRIC ACID, 1.00 Molar | FISHER SCIENTIFIC | C6H8O7, solution |
50/50 w/w Citric Acid Monohydrate in Water | PREMIX CITRIC ACID CAW 1:1 | TRANSENE COMPANY, INC. | C6H8O7, solution |
Citric acid, granular, monohydrate, 3 kg | CITRIC ACID GRAN CERT ACS 3KG Percent Purity 99.0 to 102.0% | FISHER SCIENTIFIC | C6H8O7, powder |
Acetic, 2.5L | ACETIC ACID GLACIAL ACS 2.5L IND SAF-CT Assay Percent Range: ≥99.7% w/w | FISHER SCIENTIFIC | |
Hydrochloric, 2.5L | HYDROCHLORIC ACID Percent Purity 36.5 to 38.0% (w/w) | FISHER SCIENTIFIC | HCl |
Hydrofluoric, 49%, 500 Ml | HYDROFLUORIC ACID RGT 500ML Assay (HF) 48 - 51% | VWR INTERNATIONAL | HF |
Hydrofluoric, Buffered HF, 1 gal | BUFFER-HF | TRANSENE COMPANY, INC. | BHF, "Buffered oxide etch"
4-8% HF |
Hydrobromic, 500 mL | HYDROBROMIC ACID 48% CERT ACS 500ML Percent Purity 47.0 to 49.0% | FISHER SCIENTIFIC | HBr |
Chrome mask etchant, 1 qt | CHROMIUM ETCHANT 1020 | TRANSENE COMPANY, INC. | |
Aluminum etchant, A, 1 qt | ALUMINUM ETCHANT TYPE A | TRANSENE COMPANY, INC. | |
Aluminum etchant, D, 1 qt | ALUMINUM ETCHANT TYPE D | TRANSENE COMPANY, INC. | |
Gold etchant, TFA, 1 qt | GOLD ETCHANT TFA | TRANSENE COMPANY, INC. | |
Nickel etchant, TFB, 1 qt. | NICKEL ETCH TFB | TRANSENE COMPANY, INC. | |
Titanium etchant, TFTN | TITANIUM ETCHANT TFTN | TRANSENE COMPANY, INC. | |
Nanostrip | KMG-Nanostrip | INTEGRATED MICRO MATERIALS | |
Oxalic Acid | OXALIC ACID CERTIF ACS 500G Percent Purity 99.5 to 102.5% | FISHER SCIENTIFIC | |
Formic Acid | FORMIC ACID 2.5LT 98% (ACS) | FISHER SCIENTIFIC | |
Chromic Acid (Chromium Trioxide) | Chromium Trioxide (Crystalline/Certified ACS) Percent Purity ≥98.0% | FISHER SCIENTIFIC | CrO3 |
Ammonium hydroxide, 2.5 L | AMMONIUM HYDROXIDE ACS Assay Percent Range: 28.0 to 30.0 w/w % | FISHER SCIENTIFIC | NH4OH |
Ammonium sulfide, 500 mL | AMMONIUM SULFIDE SOLUTION Assay Percent Range 20 to 24% (aqueous) | FISHER SCIENTIFIC | (NH4)2S |
Sodium hydroxide, 1L | SODIUM HYDROX SOL 50% CERT 1L Percent Purity Inclusive between 50% | FISHER SCIENTIFIC | NaOH |
Potassium hydroxide, 43. | POT HYDROX SOL 45% CERT 4L Concentration or Composition (by Analyte or Components) 45% | FISHER SCIENTIFIC | KOH |
Hydrogen peroxide, 500 mL | HYDROGEN PEROXIDE 30% Percent Purity 30.0 to 32.0% | FISHER SCIENTIFIC | H2O2 |
Hydrogen peroxide, 1 gal | HYDROGEN PEROXIDE 30% Percent Purity 30.0 to 32.0% | FISHER SCIENTIFIC | H2O2 |
TMAH, 25%, per liter | TETRAMETHYLAMMONIUM HYDROXIDE, 25% | TRANSENE COMPANY, INC. | |
Saturated Bromine Water (SBW), 1L | BROMINE WATER RGT 500ML Percent Purity ≥99.5% | FISHER SCIENTIFIC | Br2 : H2O |
AZ400k developer, concentrated, 1 gal | AZ 400K CONCENTRATE PHOTORESIST DEVELOPER | INTEGRATED MICRO MATERIALS | |
AZ400k developer, 1:4 diluted, 1 gal | AZ 400k 1:4 PHOTORESIST DEVELOPER | INTEGRATED MICRO MATERIALS | Pre-diluted |
AZ 726 MIF developer, 1 gal | AZ 726 MIF DEVELOPER | INTEGRATED MICRO MATERIALS | |
AZ NMP Rinse & Photoresist Stripper | AZ® NMP Rinse & Photoresist Stripper | INTEGRATED MICRO MATERIALS | |
AZ 300 T, stripper, 1 gal. | AZ 300T STRIPPER | INTEGRATED MICRO MATERIALS | |
MicroChem 101A Developer, 1 gal | 101A DEVELOPER | MICROCHEM CORP. | SAL 101A, XP 101A |
AZ 300 MIF Developer | AZ 300 MIF DEVELOPER | INTEGRATED MICRO MATERIALS | |
SU-8 Developer | SU-8 DEVELOPER - 4 X 4L | MICROCHEM CORP. | |
DS2100 BCB Developer | DEVELOPER DS2100 | MICROCHEM CORP. | BCB Developer |
EC 11 | EC SOLVENT 11 - 4 GL CS | MICROCHEM CORP. | |
AZ EBR | AZ EBR EDGE BEAD REMOVER | INTEGRATED MICRO MATERIALS | |
KwikStrip, gallon size | AZ KWIK STRIP PHOTORESIST STRIPPER | INTEGRATED MICRO MATERIALS | |
Remover PG, SU-8 stripper | REMOVER PG - 4 X 4L | MICROCHEM CORP. | |
SPR 955 CM-0.9, 1 Gal. | SPR 955CM-0.9 - 1 GL | MICROCHEM CORP. | Photoresist, PR |
SPR 955 CM-1.8, 1 Gal. | SPR 955CM-1.8 - 1 GL | MICROCHEM CORP. | Photoresist, PR |
SPR 220-3.0, 1 gal. | SPR 220-3.0 P.R. 1GL | MICROCHEM CORP. | Photoresist, PR |
SPR 220-7.0, 1 GAL, | SPR 220-7.0 P.R. 1GL | MICROCHEM CORP. | Photoresist, PR |
CEM-365 IS, for stepper, 1 pint. | CEM365IS-QT | SHIN-ETSU MICROSI, INC. | Photoresist, PR contrast enhancer |
OCG 825-35CS | OCG 825 35CS 1X1 GALLON GLASS | GALLADE CHEMICAL | Photoresist, PR |
AZ P4110 1Qt. | AZ P4110 PHOTORESIST | INTEGRATED MICRO MATERIALS | Photoresist, PR |
AZ P4210 1Qt. | AZ P4210 G-LINE/BROADBAND PHOTORESIST | INTEGRATED MICRO MATERIALS | Photoresist, PR |
AZ P4330 RS 1QT. | AZ P4330-RS | INTEGRATED MICRO MATERIALS | Photoresist, PR |
AZ 5214-EIR 1QT. | AZ 5214-E IR PHOTORESIST | INTEGRATED MICRO MATERIALS | Photoresist, PR |
AZ P4620 1QT | AZP4620-1Q | INTEGRATED MICRO MATERIALS | Photoresist, PR |
AZ P9260 1gal. | AZ® 9260 i-line / Broadband Photoresist | INTEGRATED MICRO MATERIALS | Photoresist, PR |
AZnLOF 2020, 1 gal. | AZ nLoF 2020 NEGATIVE TONE LIFT-OFF PHOTORESIST | INTEGRATED MICRO MATERIALS | Photoresist, PR |
AZnLOF 2035, 1 qt. | AZ Nlof 2035 NEGATIVE TONE LIFT-OFF PHOTORESIST | INTEGRATED MICRO MATERIALS | Photoresist, PR |
AZnLOF 2070, 1 qt | AZ NLOF2070 NEGATIVE TONE LIFT-OFF PHOTORESIST | INTEGRATED MICRO MATERIALS | Photoresist, PR |
NR9-1000PY | Negative Resist NR9-1000PY | Futurrex, Inc. | Photoresist, PR |
NR9-3000PY | Negative Resist NR9-3000PY | Futurrex, Inc. | Photoresist, PR |
NR9-6000PY | Negative Resist NR9-6000PY | Futurrex, Inc. | Photoresist, PR |
LOL 2000, 1 qt. | LOL 2000 -1 QT | MICROCHEM CORP. | Photoresist, PR Underlayer |
AZ nLOF P5510 photoresist, 1 gallon | AZ nLoF 5510 NEGATIVE TONE LIFT-OFF PHOTORESIST. | INTEGRATED MICRO MATERIALS | Photoresist, PR |
THMR-IP3600 HP D | THMR-IP3600 HP | TOK AMERICA, INC. | Photoresist, PR |
XHRIC-11 1 LITER | XHRIC-11 1 LITER | BREWER SCIENCE, INC. | Photoresist, PR, BARC |
MR-I 7020, Imprint Resist 250ml | MRT - mr-I 7020E - 250ml GLASS | MICROCHEM CORP. | Nanoimprint Thermoplastic Resist, NIL |
PMGI, SF 3, 500 ml | PMGI SF 3 - 500ml Glass | MICROCHEM CORP. | Photoresist, PR |
PMGI, SF 5, 500 ml | PMGI SF 5 - 500ml Glass | MICROCHEM CORP. | Photoresist, PR |
PMGI, SF 8, 500 ml | PMGI SF-8, glass 500ml | MICROCHEM CORP. | Photoresist, PR |
PMGI, SF11, 500 ml | PMGI SF 11 - 500ML GLASS | MICROCHEM CORP. | Photoresist, PR |
PMGI, SF15, 500 ml | PMGI SF 15 - 500ML GLASS | MICROCHEM CORP. | Photoresist, PR |
Dow Advanced Electronic, 4024-40, photo BCB | CYCLOTENE* 4024 - 40 / 0.95 LITERS (BCB) | MICROCHEM CORP. | Photo-BCB |
Cyclotene 3022-46 | CYCLOTENE* 3022-46 | MICROCHEM CORP. | BCB |
AP3000 BCB Adhesion Promoter, gall. | ADHESION PROMOTER AP3000 | MICROCHEM CORP. | BCB Adhesion Promoter |
Omnicoat, adhesion promoter for SU-8 | OMNICOAT - 500ML GLASS | MICROCHEM CORP. | Resist |
HMDS, (Fineline adhes.), 1 bt. | MPHP-PT MICROPRIMER HIGH PURITY | SHIN-ETSU MICROSI, INC. | Photoresist Adhesion Promoter |
Tergitol | Spectrum Chemical Manufacturing Corporation TERGITOL NP-10 SURFCTNT 500ML T1273500ML | FISHER SCIENTIFIC | Detergent |
SU-8 2005 Photoresist | SU-8 2005 - 500ml GLASS | MICROCHEM CORP. | Photoresist, PR |
SU-8 2010 Photoresist | SU-8 2010 - 500ml GLASS | MICROCHEM CORP. | Photoresist, PR |
SU-8 2015 Photoresist | SU-8 2015 - 500ml GLASS | MICROCHEM CORP. | Photoresist, PR |
SU-8 2075 Photoresist | SU-8 2075 - 500ml Glass Resist | MICROCHEM CORP. | Photoresist, PR |
UV-6 0.8 Photoresist | UV6-0.8 | MICROCHEM CORP. | Photoresist, PR |
DUV42P-6 | DUV42P-6 | BREWER SCIENCE, INC | Photoresist, PR, BARC |
Honeywell 512B spin-on-glass, 125 ml. | ACCUGLASS 512B SPIN-ON GLASS | HONEYWELL ANALYTICS INC. | SOG |
UVN 30-0.8L (UVN 2300-0.5) | UVN 30-0.8L-1 GL NOWPAK | MICROCHEM CORP. | Photoresist, PR |
Brewer Science DS-K101-304, 1 gal bt. | ARC DS-K101-304, 1 LITER | BREWER SCIENCE, INC. | Photoresist, PR, BARC |
UV 210GS-0.3, 1 gal. bt. | UV 210GS-0.3 - 1 GL NOWPAK | MICROCHEM CORP. | Photoresist, PR |
mr-UV Cur 21 100 nm, 100ml. | MRT-mr-UV Cur 21, 100nm - 100ml Glass | MICROCHEM CORP. | Nanoimprint Resist |
Santovac 5P | Santovac 5P Ultra Polyphenyl Ether Pump Fluid | KURT J LESKER | Oil |
SF1 Polishing Fluid | SF1 Polishing Fluid | LOGITECH LIMITED | CMP Slurry |