Stepper 3 (ASML DUV)
Revision as of 06:59, 11 July 2012 by Zwarburg (talk | contribs) (moved Stepper 3 (ASML) to Stepper 3 (ASML DUV))
The printable version is no longer supported and may have rendering errors. Please update your browser bookmarks and please use the default browser print function instead.
|
About
The ASML DUV stepper is a 248nm line stepper for imaging dense features down to below 200nm and isolated line structures down to below 150nm. The system is a variable NA system and has a field image size of 21 x 21mm for 0.63 NA and a field size of 22mm x 27mm for 0.4 to 0.57NA. Overlay accuracy is better than 30nm. The system is configured for 4” wafers and pieces down to 14mm in size can be exposed using a 4” wafer as a carrier.