- ALD-Al2O3-Plasma-300C-Recipe.pdf ; 992 KB
- ALD-AlN-300-recipe.pdf ; 1.09 MB
- ALD-HfO2-100-recipe.pdf ; 1.09 MB
- ALD-HfO2-300-recipe.pdf ; 1.08 MB
- ALD-Operating-Instrucitons.pdf ; 68 KB
- ALD-SiO2-100-recipe.pdf ; 1.08 MB
- ALD-SiO2-300-recipe.pdf ; 1.09 MB
- ALD-ZrO2-300-recipe.pdf ; 1.08 MB
- ALD operating instructions-1.pdf ; 66 KB
- AR2-Anti-Reflective-Coating.pdf ; 91 KB
- ARC etch + Cr etch - UV6 at 2krpm (900nm) survived v2 - screenshot.jpg 1,280 × 1,024; 294 KB
- ASML CD Cals - Example Plot.jpg 397 × 240; 32 KB
- ASML CD Cals - Example Table.jpg 855 × 454; 100 KB
- ASML IQC Focus Mean Correction screenshot.jpg 890 × 490; 165 KB
- ASML Job Set-Up Guide.pdf ; 3.13 MB
- ASML Job Set-Up Guide simple v1.pdf ; 1.6 MB
- ASML Job Set-Up Guide v2.pdf ; 1.81 MB
- ASML Mask Making Guidelines.pdf ; 176 KB
- ASML On Wafer Mark.gds ; 4 KB
- ASML Stepper 3 - HELP button error log screenshot.png 768 × 726; 54 KB
- AXP4000pb-Datasheet.pdf ; 1.86 MB
- AZ300MIF-Developer-Datasheet.pdf ; 77 KB
- AZ300T-Resist-Remover.pdf ; 383 KB
- AZ400K-Developer-Datasheet.pdf ; 77 KB
- AZ5214-Negative-Resist-Datasheet.pdf ; 101 KB
- AZ NMP RINSE MSDS.pdf ; 285 KB
- AZnLOF2020contactrecipe.pdf ; 450 KB
- Adv. PECVD2-STD SiO2.xlsx ; 783 KB
- Adv. PECVD2- STD LSNitride2.xlsx ; 944 KB
- Adv. PECVD2- STD Nitride2.xlsx ; 1.31 MB
- AdvPECVD2LSNdep2.jpg 4,032 × 3,024; 1.68 MB
- Adv PECVD LS NITRIDE2 April 2014.pdf ; 122 KB