User contributions
Jump to navigation
Jump to search
- 13:24, 9 July 2012 diff hist -47 Vacuum Deposition Recipes →Recipes
- 13:23, 9 July 2012 diff hist +664 Vacuum Deposition Recipes →Plasma Enhanced Chemical Vapor Deposition (PECVD)
- 13:16, 9 July 2012 diff hist +52 Vacuum Deposition Recipes
- 13:14, 9 July 2012 diff hist +26 Vacuum Deposition Recipes
- 13:14, 9 July 2012 diff hist +11 Tool List
- 13:11, 9 July 2012 diff hist +527 Vacuum Deposition Recipes
- 13:08, 9 July 2012 diff hist +560 Vacuum Deposition Recipes →Plasma Enhanced Chemical Vapor Deposition (PECVD)
- 12:13, 9 July 2012 diff hist +1 Tool List →Dry Etch
- 12:13, 9 July 2012 diff hist +14 Tool List →Vacuum Deposition
- 11:42, 9 July 2012 diff hist -43 Lab Rules OLD 2018 →Communications and Internet Access
- 10:56, 9 July 2012 diff hist -88 Lab Rules OLD 2018 →Preparing Equipment for Entry into the Nanofab
- 10:45, 9 July 2012 diff hist +25 Vacuum Deposition Recipes →Recipe 1
- 10:44, 9 July 2012 diff hist +40 Vacuum Deposition Recipes
- 10:44, 9 July 2012 diff hist +30 Vacuum Deposition Recipes →E-Beam Evaporation
- 10:42, 9 July 2012 diff hist -114 Lab Rules OLD 2018 →General Nanofab Information
- 10:36, 9 July 2012 diff hist -3 Biljana Stamenic
- 10:36, 9 July 2012 diff hist -32 Biljana Stamenic
- 10:34, 9 July 2012 diff hist -30 Lab Rules OLD 2018 →Film
- 10:33, 9 July 2012 diff hist +454 Lab Rules OLD 2018 →Nanofab Apparel and Gloves
- 10:28, 9 July 2012 diff hist -9 Lab Rules OLD 2018 →Chemical Waste Disposal
- 10:26, 9 July 2012 diff hist -234 Lab Rules OLD 2018
- 10:20, 9 July 2012 diff hist +34,117 N Lab Rules OLD 2018 Created page with "While working in the Nanofab, you are surrounded by dangerous and deadly chemicals, gases, high voltages, radiation, and mechanical systems. The responsibility lies with users a…"
- 18:50, 3 July 2012 diff hist +22 Biljana Stamenic
- 19:26, 2 July 2012 diff hist +30 Staff List
- 17:28, 2 July 2012 diff hist +2 ICP-PECVD (Unaxis VLR)
- 17:28, 2 July 2012 diff hist +1 ICP-Etch (Unaxis VLR)
- 17:25, 2 July 2012 diff hist 0 N File:UnaxisICPInstructions.pdf current
- 17:24, 2 July 2012 diff hist +77 ICP-Etch (Unaxis VLR) →Detailed Specifications
- 17:21, 2 July 2012 diff hist +98 ICP-Etch (Unaxis VLR)
- 17:19, 2 July 2012 diff hist +1,445 N ICP-Etch (Unaxis VLR) Created page with "{{tool|{{PAGENAME}} |picture=UnaxisICP.jpg |type = Dry Etch |super= Tony Bosch |phone=(805)839-3918x217 |location=Bay 1 |email=bosch@ece.ucsb.edu |description = ? |manufacturer =…"
- 16:22, 2 July 2012 diff hist +1 E-Beam 3 (Temescal)
- 11:52, 2 July 2012 diff hist +48 Template:Nav
- 11:50, 2 July 2012 diff hist -14 Template:Links
- 11:50, 2 July 2012 diff hist +13 N File:StripAnnealer.jpg {{toolimage}} current
- 11:49, 2 July 2012 diff hist +1,187 N Strip Annealer Created page with "{{tool|{{PAGENAME}} |picture=StripAnnealer.jpg |type = Thermal Processing |super= Tony Bosch |phone=(805)839-3918x217 |location=Bay 5 |email=bosch@ece.ucsb.edu |description = Str…"
- 11:44, 2 July 2012 diff hist -43 MediaWiki:Sidebar
- 11:43, 2 July 2012 diff hist +82 MediaWiki:Sidebar
- 11:42, 2 July 2012 diff hist +16 N Thermal Processing Recipes Created page with ".... =Recipes="
- 11:42, 2 July 2012 diff hist +16 N Wet Etching Recipes Created page with ".... =Recipes="
- 11:40, 2 July 2012 diff hist +248 N Lithography Recipes Created page with "{{WIP}} *ASML Recipes *GCA Stepper Recipes *Contact Lithography Recipes *Nanoimprint Recipes *Optical Bi-Layer Recipes *E-Beam Lithography Recipes …"
- 11:40, 2 July 2012 diff hist +79 MediaWiki:Sidebar
- 11:39, 2 July 2012 diff hist +3,822 N Dry Etching Recipes Created page with "{| border="1" class="collapsible wikitable" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" |-bgcolor="#D0E7FF" ! colspan=10 height…"
- 11:37, 2 July 2012 diff hist +2 Vacuum Deposition Recipes →Recipes
- 11:37, 2 July 2012 diff hist +49 Vacuum Deposition Recipes
- 11:36, 2 July 2012 diff hist +1 Vacuum Deposition Recipes →=E-Beam Evaporation
- 11:36, 2 July 2012 diff hist +220 Vacuum Deposition Recipes →Recipes
- 11:34, 2 July 2012 diff hist +20 Vacuum Deposition Recipes
- 11:34, 2 July 2012 diff hist +12,511 N Vacuum Deposition Recipes Created page with "{| border="1" class="collapsible wikitable" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center;" |-bgcolor="#D0E7FF" ! colspan=18 height=45 width=1575|…"
- 11:32, 2 July 2012 diff hist -30 MediaWiki:Sidebar
- 11:32, 2 July 2012 diff hist +1 MediaWiki:Sidebar
- 11:32, 2 July 2012 diff hist +29 MediaWiki:Sidebar
- 11:32, 2 July 2012 diff hist -66 MediaWiki:Sidebar
- 11:30, 2 July 2012 diff hist -44 MediaWiki:Sidebar
- 11:28, 2 July 2012 diff hist +288 Template:Nav
- 11:24, 2 July 2012 diff hist +13 N File:WaferThermco.jpg {{toolimage}} current
- 11:24, 2 July 2012 diff hist +1,067 N Tube Furnace Wafer Bonding (Thermco) Created page with "{{tool|{{PAGENAME}} |picture=WaferThermco.jpg |type = Thermal Processing |super= Mike Silva |phone=(805)839-3918x219 |location=Bay 4 |email=silva@ece.ucsb.edu |description = Wafe…"
- 07:52, 2 July 2012 diff hist +13 N File:RTP.jpg {{toolimage}} current
- 07:51, 2 July 2012 diff hist -3 Rapid Thermal Processor (AET RX6)
- 07:49, 2 July 2012 diff hist +2,079 Rapid Thermal Processor (AET RX6)
- 07:40, 2 July 2012 diff hist +1,035 N Probe Station & Curve Tracer Created page with "{{tool|{{PAGENAME}} |picture=ProbeStation.jpg |type = Inspection, Test and Characterization |super= Tony Bosch |phone=(805)839-3918x217 |location=Bay 4 |email=bosch@ece.ucsb.edu …"
- 07:38, 2 July 2012 diff hist +13 N File:Dektak6M.jpg {{toolimage}} current
- 07:37, 2 July 2012 diff hist +1,651 N Step Profilometer (DektakXT) Created page with "{{tool|{{PAGENAME}} |picture=Dektak6M.jpg |type = Inspection, Test and Characterization |super= Mike Silva |phone=(805)839-3918x219 |location=Bay 3 |email=silva@ece.ucsb.edu |des…"
- 13:14, 1 July 2012 diff hist +13 N File:Dektak2A.jpg {{toolimage}} current
- 12:16, 1 July 2012 diff hist +8 N File:TartaricAcidMSDS.pdf {{MSDS}} current
- 12:15, 1 July 2012 diff hist +8 N File:SulfuricAcidFuming.pdf {{MSDS}} current
- 12:15, 1 July 2012 diff hist +8 N File:SulfuricAcid93%MSDS.pdf {{MSDS}} current
- 12:15, 1 July 2012 diff hist +8 N File:SulfamicAcidMSDS.pdf {{MSDS}} current
- 12:15, 1 July 2012 diff hist +8 N File:SuccinicAcid99%MSDS.pdf {{MSDS}} current
- 12:15, 1 July 2012 diff hist +278 Chemical List - OLD 2018-09-05 →Acids
- 12:11, 1 July 2012 diff hist +7 N File:SelenousAcidMSDS.pdf {{MSDS}
- 12:11, 1 July 2012 diff hist +7 N File:OxalicAcidDihydrateMSDS.pdf {{MSDS}
- 12:11, 1 July 2012 diff hist +7 N File:MethacrylicAcidMSDS.pdf {{MSDS}
- 12:10, 1 July 2012 diff hist +7 N File:LacticAcidMSDS.pdf {{MSDS}
- 12:10, 1 July 2012 diff hist +7 N File:LacticAcidFractionalMSDS.pdf {{MSDS}
- 12:10, 1 July 2012 diff hist +7 N File:HydroiodicAcidMSDS.pdf {{MSDS}
- 12:09, 1 July 2012 diff hist +359 Chemical List - OLD 2018-09-05 →Acids
- 12:02, 1 July 2012 diff hist +8 N File:FormicAcidMSDS.pdf {{MSDS}} current
- 12:02, 1 July 2012 diff hist +8 N File:BoricAcidMSDS.pdf {{MSDS}} current
- 12:01, 1 July 2012 diff hist +96 Chemical List - OLD 2018-09-05 →Acids
- 11:33, 1 July 2012 diff hist +1,725 N Sputter 2 (SFI Endeavor) Created page with "{{tool|{{PAGENAME}} |picture=Sputter2.jpg |type = Vacuum Deposition |super= Brian Lingg |phone=(805)839-3918x210 |location=Bay 1 |email=lingg@ece.ucsb.edu |description = 3 chambe…"
- 11:25, 1 July 2012 diff hist +722 N Resistivity Mapper (CDE RESMAP) Created page with "{{tool|{{PAGENAME}} |picture=CDEResmap.jpg |type = Inspection, Test and Characterization |super= Tony Bosch |phone=(805)839-3918x217 |location=Bay ? |email=bosch@ece.ucsb.edu |de…"
- 11:19, 1 July 2012 diff hist +13 N File:VeecoNanoman.jpg {{toolimage}}
- 09:57, 1 July 2012 diff hist 0 Optical Film Thickness (Nanometric)
- 09:54, 1 July 2012 diff hist 0 Tool List →Inspection, Test and Characterization
- 09:54, 1 July 2012 diff hist +994 N Film Stress (Tencor Flexus) Created page with "{{tool|{{PAGENAME}} |picture=Tencor.jpg |type = Inspection, Test and Characterization |super=Mike Silva |phone=(805)839-3918x219 |location=Bay ? |email=silva@ece.ucsb.edu |descri…"
- 09:49, 1 July 2012 diff hist +1,087 N Optical Film Thickness (Filmetrics) Created page with "{{tool|{{PAGENAME}} |picture=Filmmetrics.jpg |type = Inspection, Test and Characterization |super= Tony Bosch |phone=(805)839-3918x217 |location=Bay ? |email=bosch@ece.ucsb.edu |…"
- 09:31, 1 July 2012 diff hist +1,055 N Ellipsometer (Woollam) Created page with "{{tool|{{PAGENAME}} |picture = Woollam.jpg |type = Inspection, Test and Characterization |super = Brian Thibeault |phone = (805)839-2268 |email = thibeault@ece.ucsb.edu |locatio…"
- 09:17, 1 July 2012 diff hist +16 Template:Tool
- 09:16, 1 July 2012 diff hist +84 Template:Tool
- 09:16, 1 July 2012 diff hist 0 File:OlympusLEXT.jpg uploaded a new version of "File:OlympusLEXT.jpg": removed border current
- 09:15, 1 July 2012 diff hist +13 N File:OlympusLEXT.jpg {{toolimage}}
- 09:15, 1 July 2012 diff hist +664 N Laser Scanning Confocal M-scope (Olympus LEXT) Created page with "{{tool|{{PAGENAME}} |picture=OlympusLEXT.jpg |type = Inspection, Test and Characterization |super= Tony Bosch |phone=(805)839-3918x217 |location=Bay 4 |email=bosch@ece.ucsb.edu |…"
- 09:13, 1 July 2012 diff hist +23 Optical Film Thickness (Nanometric)
- 09:13, 1 July 2012 diff hist -1 Optical Film Thickness (Nanometric)
- 09:12, 1 July 2012 diff hist +13 N File:Nanometric.jpg {{toolimage}}
- 09:12, 1 July 2012 diff hist +1,587 N Optical Film Thickness (Nanometric) Created page with "{{tool|{{PAGENAME}} |picture=Nanometric.jpg |type = Wet Processing |super= Tony Bosch |phone=(805)839-3918x217 |location=Bay ? |email=bosch@ece.ucsb.edu |description = Reflectome…"
- 08:37, 1 July 2012 diff hist +13 N File:QFI.jpg {{toolimage}} current
- 08:32, 1 July 2012 diff hist +1,582 N IR Thermal Microscope (QFI) Created page with "{{tool|{{PAGENAME}} |picture=QFI.jpg |type = Inspection, Test and Characterization |super= Brian Lingg |phone=(805)839-3918x210 |location=Bay 2 |email=lingg@ece.ucsb.edu |descrip…"
- 08:30, 1 July 2012 diff hist -1 PECVD 1 (PlasmaTherm 790)
- 08:29, 1 July 2012 diff hist +1,041 N Field Emission SEM 2 (JEOL IT800SHL) Created page with "{{tool|{{PAGENAME}} |picture=JeolFesem.jpg |type = Inspection, Test and Characterization |super= Bill Mitchell |phone= (805)893-4974 |location=Bay 1 |email=mitchell@ece.ucsb.edu …"