User contributions
Jump to navigation
Jump to search
- 08:44, 2 September 2022 diff hist +59 Oxford ICP Etcher - Process Control Data →Process Control Data - InP Ridge Etch (Oxford ICP Etcher) Tag: Visual edit
- 18:12, 1 September 2022 diff hist +232 Test Data of etching SiO2 with CHF3/CF4-ICP1 Tag: Visual edit
- 18:09, 1 September 2022 diff hist 0 N File:CS pan1 090122 002.jpg current
- 18:09, 1 September 2022 diff hist 0 N File:30D pan1 090122 001.jpg current
- 18:06, 1 September 2022 diff hist +229 Oxford ICP Etcher - Process Control Data Tag: Visual edit
- 18:04, 1 September 2022 diff hist 0 N File:CS oxford 090122 002.jpg current
- 18:04, 1 September 2022 diff hist 0 N File:30D oxford 090122 002.jpg current
- 18:16, 26 August 2022 diff hist +230 Test Data of etching SiO2 with CHF3/CF4 Tag: Visual edit
- 18:14, 26 August 2022 diff hist 0 N File:30D Pan2 082622 001.jpg current
- 18:13, 26 August 2022 diff hist 0 N File:CS Pan2 082622 001.jpg current
- 18:12, 26 August 2022 diff hist +251 Test Data of Etching SiO2 with CHF3/CF4-Fluorine ICP Etcher Tag: Visual edit
- 18:06, 26 August 2022 diff hist 0 N File:30D FICP 082622 001.jpg current
- 18:05, 26 August 2022 diff hist 0 N File:CS FICP 082622 001.jpg current
- 18:54, 22 August 2022 diff hist +285 Test Data of etching SiO2 with CHF3/CF4-ICP1 Tag: Visual edit
- 18:51, 22 August 2022 diff hist 0 N File:CS Pan1 082222 002.jpg current
- 18:50, 22 August 2022 diff hist 0 N File:45D Pan1 082222 001.jpg current
- 18:49, 22 August 2022 diff hist +255 Test Data of Etching SiO2 with CHF3/CF4-Fluorine ICP Etcher new trial Tag: Visual edit
- 18:46, 22 August 2022 diff hist 0 N File:CS FICP 082222 002.jpg current
- 18:45, 22 August 2022 diff hist 0 N File:40D FICP 082222 001.jpg current
- 17:14, 19 August 2022 diff hist +9 Test Data of etching SiO2 with CHF3/CF4 Tag: Visual edit
- 17:10, 19 August 2022 diff hist +226 Test Data of etching SiO2 with CHF3/CF4 Tag: Visual edit
- 17:10, 19 August 2022 diff hist 0 N File:CS 08082022 pan2 001.jpg current
- 17:09, 19 August 2022 diff hist 0 N File:30D 08082022 pan2 001.jpg current
- 17:07, 19 August 2022 diff hist +5 Test Data of Etching SiO2 with CHF3/CF4-Fluorine ICP Etcher Tag: Visual edit
- 17:07, 19 August 2022 diff hist +7 Test Data of etching SiO2 with CHF3/CF4-ICP1 Tag: Visual edit
- 17:06, 19 August 2022 diff hist +9 Test Data of etching SiO2 with CHF3/CF4-ICP1 Tag: Visual edit
- 17:04, 19 August 2022 diff hist +220 Test Data of etching SiO2 with CHF3/CF4-ICP1 Tag: Visual edit
- 17:00, 19 August 2022 diff hist 0 N File:CS 08052022 pan1 001.jpg current
- 16:59, 19 August 2022 diff hist 0 N File:30D 08052022 pan1 001.jpg current
- 16:58, 19 August 2022 diff hist +253 Test Data of Etching SiO2 with CHF3/CF4-Fluorine ICP Etcher Tag: Visual edit
- 16:52, 19 August 2022 diff hist 0 N File:CS 08192022 FICP 001.jpg current
- 16:51, 19 August 2022 diff hist 0 N File:30D 08192022 FICP 001.jpg current
- 16:47, 19 August 2022 diff hist -13 Oxford ICP Etcher - Process Control Data Tag: Visual edit
- 16:47, 19 August 2022 diff hist +67 N File:InP 07012022 CS 001 copy.jpg Jenky image, but "corrected" date to make it 7/1/2022 current
- 17:25, 12 August 2022 diff hist +76 Oxford ICP Etcher - Process Control Data updated Tag: Visual edit
- 17:18, 12 August 2022 diff hist +32 N File:A734DC5E-639E-4FDC-8F30-6F463470BC27.jpeg InP Etch 8/01/2022 current
- 17:56, 1 August 2022 diff hist +6 Oxford ICP Etcher - Process Control Data Tag: Visual edit
- 17:53, 1 August 2022 diff hist +9 Test Data of etching SiO2 with CHF3/CF4 Tag: Visual edit
- 17:52, 1 August 2022 diff hist 0 N File:CS 002 07-29-22.jpg current
- 17:50, 1 August 2022 diff hist +7 Oxford ICP Etcher - Process Control Data added correct picture Tag: Visual edit
- 17:49, 1 August 2022 diff hist +124 File:45D 001 8-1-22.jpg messed up file name, couldn't figure out how to delete file from wiki so I needed to explain here. current Tag: Visual edit
- 17:46, 1 August 2022 diff hist 0 N File:45D 001 8-1-22.jpg
- 17:44, 1 August 2022 diff hist +195 Oxford ICP Etcher - Process Control Data added data for 8/1 etch cal Tag: Visual edit
- 17:43, 1 August 2022 diff hist 0 File:45D 001.jpg Noahdutra uploaded a new version of File:45D 001.jpg current
- 17:42, 1 August 2022 diff hist 0 File:CS 002.jpg Noahdutra uploaded a new version of File:CS 002.jpg current
- 17:37, 1 August 2022 diff hist +177 Oxford ICP Etcher - Process Control Data added 45d picture for july 1st etch Tag: Visual edit
- 17:33, 1 August 2022 diff hist +42 N File:45D 001.jpg Oxford InP 45D, no NH4OH dip
- 18:19, 29 July 2022 diff hist +208 Test Data of etching SiO2 with CHF3/CF4 added etch data for 7/29 Tag: Visual edit
- 18:17, 29 July 2022 diff hist +40 N File:CS 002.jpg SiO2 Etch Pan 2 07/29/2022
- 18:16, 29 July 2022 diff hist +36 N File:30D 002.jpg SiO2 Pan2 etch 7/29/22 current
- 18:11, 29 July 2022 diff hist +208 Test Data of etching SiO2 with CHF3/CF4-ICP1 added etch data for 7/27 Tag: Visual edit
- 18:10, 29 July 2022 diff hist +37 N File:30D 001.jpg SiO2 Etch Pan 1 7/27/22 current
- 18:08, 29 July 2022 diff hist +34 N File:CS 004.jpg SiO2 Pan 1 etch 2/27 current
- 16:50, 18 July 2022 diff hist +90 Test Data of etching SiO2 with CHF3/CF4 Added CS Tag: Visual edit
- 16:49, 18 July 2022 diff hist 0 N File:ND Pan2 071522 CS.jpg current
- 16:48, 18 July 2022 diff hist +139 Test Data of etching SiO2 with CHF3/CF4 added 45d picture 7/15/22 Tag: Visual edit
- 16:47, 18 July 2022 diff hist 0 N File:ND Pan2 071522 45D.jpg current