Difference between revisions of "Resistivity Mapper (CDE RESMAP)"
Jump to navigation
Jump to search
Millerski w (talk | contribs) (Updated SOP) |
|||
(5 intermediate revisions by 3 users not shown) | |||
Line 1: | Line 1: | ||
− | {{ |
+ | {{tool2|{{PAGENAME}} |
|picture=CDEResmap.jpg |
|picture=CDEResmap.jpg |
||
|type = Inspection, Test and Characterization |
|type = Inspection, Test and Characterization |
||
− | |super= |
+ | |super= Bill Millerski |
+ | |super2= Tony Bosch |
||
|phone=(805)839-3918x217 |
|phone=(805)839-3918x217 |
||
|location=Bay ? |
|location=Bay ? |
||
Line 10: | Line 11: | ||
|materials = |
|materials = |
||
}} |
}} |
||
− | = |
+ | =About= |
− | The CDE Resmap 4 point resistivity mapper is used for measuring resistivity across the wafer for substrates and thin films deposited in the facility. The system can do automated resistivity mapping for pieces to 8 inch wafers. |
+ | The CDE Resmap 4 point resistivity mapper is used for measuring resistivity across the wafer for substrates and thin films deposited in the facility. The system can do automated resistivity mapping for pieces to 8 inch wafers. |
+ | |||
+ | The resistivity range is 2 mOhm/Square to 5 MOhm/square. Contour plots, 3D plots, histograms, data exporting are supported from the Windows XP based control system. |
||
+ | |||
+ | ==Instructions== |
||
+ | |||
+ | *[[CDE ResMap Quick-Start instructions]] |
||
+ | *[https://wiki.nanofab.ucsb.edu/w/images/3/37/CDE_ResMap_Operating_Instructions.pdf CDE ResMap Operating Instructions] |
||
+ | *System can export CSV files - contact supervisor for instructions. |
Latest revision as of 15:07, 30 October 2023
|
About
The CDE Resmap 4 point resistivity mapper is used for measuring resistivity across the wafer for substrates and thin films deposited in the facility. The system can do automated resistivity mapping for pieces to 8 inch wafers.
The resistivity range is 2 mOhm/Square to 5 MOhm/square. Contour plots, 3D plots, histograms, data exporting are supported from the Windows XP based control system.
Instructions
- CDE ResMap Quick-Start instructions
- CDE ResMap Operating Instructions
- System can export CSV files - contact supervisor for instructions.